Patents
US 9,969,622 B2#45373430 Most CitedActiveUnited States (USPTO)Utility

Ternary tungsten boride nitride films and methods for forming same

2Forward Citations (#45373430 Global)
0.2/yrCitation Velocity (#29483025 Global)
0.86Citation PageRank (#49945414 Global)
46Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Ternary tungsten boride nitride (WBN) thin films and related methods of formation are provided. The films are have excellent thermal stability, tunable resistivity and good adhesion to oxides. Methods of forming the films can involve thermal atomic layer deposition (ALD) processes in which boron-containing, nitrogen-containing and tungsten-containing reactants are sequentially pulsed into a reaction chamber to deposit the WBN films. In some embodiments, the processes include multiple cycles of boron-containing, nitrogen-containing and tungsten-containing reactant pulses, with each cycle including multiple boron-containing pulses.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 46 · Forward citations: 2.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method comprising: performing multiple cycles of sequentially introducing pulses of a boron-containing reactant, a nitrogen-containing reactant and a tungsten-containing reactant into a reaction chamber containing a semiconductor substrate to thereby deposit a ternary tungsten boride nitride film on the substrate, wherein the ternary tungsten boride nitride film contains tungsten-boron bonds and tungsten-nitrogen bonds, wherein a ratio of the number of boron-containing reactant pulses to the number of tungsten-containing reactant pulses introduced during the multiple cycles is at least three

  2. Claim 2Depends on #1

    The method of claim 1 , wherein each cycle comprises multip

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (46)

PatentTitleYearCitations
JP S5629648 AHigh hardness sintered body—23
US 5,633,200 AProcess for manufacturing a large grain tungsten nitride film and process for manufacturing a lightly nitrided titanium salicide diffusion barrier with a large grain tungsten nitride cover layer1997135
US 5,916,634 AChemical vapor deposition of W-Si-N and W-B-N199954
US 2001007797 A1Method of forming a tungsten plug in a semiconductor device—20
US 6,284,316 B1Chemical vapor deposition of titanium200121
US 6,287,965 B1Method of forming metal layer using atomic layer deposition and semiconductor device having the metal layer as barrier metal layer or upper or lower electrode of capacitor2001432
US 6,340,629 B1Method for forming gate electrodes of semiconductor device using a separated WN layer200243
US 2002090811 A1Method of fabricating metal lines in a semiconductor device—61
US 6,491,978 B1Deposition of CVD layers for copper metallization using novel metal organic chemical vapor deposition (MOCVD) precursors2002122
US 2002190379 A1W-CVD with fluorine-free tungsten nucleation—38
US 2003013300 A1Method and apparatus for depositing tungsten after surface treatment to improve film characteristics—39
US 2003082902 A1Semiconductor-device fabrication method—44
JP 2003193233 AMethod for depositing tungsten film—52
US 2003194850 A1Method and apparatus for improved electroplating fill of an aperture—35
US 2003224217 A1Metal nitride formation—43
US 2008081452 A1Method of forming tungsten polymetal gate having low resistance—10
US 2008124926 A1Methods for growing low-resistivity tungsten film—26
US 2008283844 A1Method for manufacturing a field effect transistor having a field plate—22
US 2009050937 A1Semiconductor device and method for manufacturing semiconductor device—9
US 2009142509 A1Hard coating excellent in sliding property and method for forming same—12
US 2010007797 A1Digital Video Fingerprinting Based on Resultant Weighted Gradient Orientation Computation—38
US 2010062149 A1Method for tuning a deposition rate during an atomic layer deposition process—21
US 2010072623 A1Semiconductor device with improved contact plugs, and related fabrication methods—18
US 2010244260 A1Semiconductor device and method for fabricating the same—11
CN 101,899,649 AMethod for forming tungsten film—7
US 2011151670 A1Method of controlling etch microloading for a tungsten-containing layer—22
US 2012077342 A1Systems and methods for selective tungsten deposition in vias—21
US 2012225192 A1Apparatus And Process For Atomic Layer Deposition—14

Non-Patent Literature (5)

  • Chinese Fifth Office Action dated May 5, 2015 issued in Application No. 200980133560.1.
  • Chinese First Office Action dated Mar. 18, 2016 issued in Application No. CN 201380022693.8.
  • Chinese First Office Action dated Sep. 6, 2015 issued in Application No. CN 201310320848.8.
  • Chinese Office Action [no translation] dated Feb. 26, 2016, issued in CN 201380022648.2.
  • Chinese Office Action [no translation] dated Sep. 6, 2015 issued in CN 201310320848.8.