Hardmask layer for 3D NAND staircase structure in semiconductor applications

2Forward Citations (#37253285 Global)
0.3/yrCitation Velocity (#26447268 Global)
1.12Citation PageRank (#35813636 Global)
44Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Embodiments of the present disclosure provide an apparatus and methods for forming a hardmask layer that may be utilized to transfer patterns or features to a film stack with accurate profiles and dimension control for manufacturing three dimensional (3D) stacked semiconductor devices. In one embodiment, a method of forming a hardmask layer on a substrate includes forming a seed layer comprising boron on a film stack disposed on a substrate by supplying a seed layer gas mixture in a processing chamber, forming a transition layer comprising born and tungsten on the seed layer by supplying a transition layer gas mixture in the processing chamber, and forming a bulk hardmask layer on the transition layer by supplying a main deposition gas mixture in the processing chamber.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 44 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming a hardmask layer on a substrate comprises: forming a seed layer comprising boron on a film stack disposed on a substrate by supplying a seed layer gas mixture in a processing chamber, wherein the seed layer gas mixture comprises at least a boron containing gas and a nitrogen containing gas; forming a gradient transition layer comprising boron and tungsten on the seed layer by supplying a transition layer gas mixture in the same processing chamber, wherein the transition layer gas mixture is supplied to the processing chamber by ramping down a gas flow rate of the boron cont

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (44)

PatentTitleYearCitations
US 5,236,550 AMethod for plasma etch of ruthenium199323
US 5,407,855 AProcess for forming a semiconductor device having a reducing/oxidizing conductive material199578
US 5,821,169 AHard mask method for transferring a multi-level photoresist pattern1998128
US 6,331,483 B1Method of film-forming of tungsten200113
US 2006024948 A1Method of fabricating dual damascene interconnection—46
US 7,109,098 B1Semiconductor junction formation process including low temperature plasma deposition of an optical absorption layer and high speed optical annealing200630
US 2006264060 A1Low temperature plasma deposition process for carbon layer deposition—40
US 2006263540 A1Process for low temperature plasma deposition of an optical absorption layer and high speed optical annealing—11
US 2006260545 A1Low temperature absorption layer deposition and high speed optical annealing system—30
US 2007026685 A1Mask structure, method of forming the mask structure, method of forming a pattern using the mask structure and method of forming contacts in a semiconductor device using the mask structure—9
US 2007032054 A1Semiconductor substrate process using a low temperature deposited carbon-containing hard mask—40
US 2007032082 A1Semiconductor substrate process using an optically writable carbon-containing mask—16
US 2007032095 A1Copper conductor annealing process employing high speed optical annealing with a low temperature-deposited optical absorber layer—40
US 2007032004 A1Copper barrier reflow process employing high speed optical annealing—20
US 2007231010 A1Electron emission element, charging device, process cartridge, and image forming apparatus—21
US 7,312,148 B2Copper barrier reflow process employing high speed optical annealing200718
US 7,312,162 B2Low temperature plasma deposition process for carbon layer deposition200724
US 7,323,401 B2Semiconductor substrate process using a low temperature deposited carbon-containing hard mask200834
US 7,335,611 B2Copper conductor annealing process employing high speed optical annealing with a low temperature-deposited optical absorber layer200813
US 7,422,775 B2Process for low temperature plasma deposition of an optical absorption layer and high speed optical annealing200818
US 7,429,532 B2Semiconductor substrate process using an optically writable carbon-containing mask200821
US 2008292798 A1Boron nitride and boron nitride-derived materials deposition method—69
US 2009078676 A1METHOD FOR DRY ETCHING Al2O3 FILM—7
US 2012264306 A1Method of Forming Opening on Semiconductor Substrate—23
US 2013014979 A1Connector Structures and Methods—20
US 2013014978 A1Electrical Barrier Layers—14
US 2014027664 A1Ternary tungsten boride nitride films and methods for forming same—16
US 8,647,989 B2Method of forming opening on semiconductor substrate20141