Abstract

Titanium alloy containing iron, that is, iron-containing titanium alloy having high strength and hardness in which iron in a composition which cannot be realized in a conventional method, is contained with no segregation, and is provided in lower cost. The α+β titanium alloy or β titanium alloy is produced by a forming process such as hot extrusion of titanium alloy powder containing 3 to 15 mass % of iron powder. The method for production of the α+β titanium alloy or β titanium alloy includes a step of mixing 3 to 15 mass % of iron powder and titanium alloy powder as the remainder, and a step of performing a forming process of hot extrusion on this powder mixture.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    α+β titanium alloy or β titanium alloy consisting of 5.1 to 5.4 mass % of aluminum, 3.4 to 3.6 mass % of vanadium, 10 to 15 mass % of iron, titanium as a remainder and inevitable impurities, wherein a deformation resistance of the titanium alloy at 900 to 980° C. in a compression test is 260 to 500 MPa.

  2. Claim 2Depends on #1

    α+β titanium alloy or β titanium alloy according to claim 1 , wherein the titanium alloy is produced by hot extrusion of titanium alloy powder containing aluminum and vanadium mixed with iron powder, and wherein the titanium alloy powder except for the iron powder is produced by a hydrogenation-dehydrogenation method.

  3. Claim 3Depends on #1

    α+β titanium alloy or β titanium alloy according to claim 1 , wherein an average concentration of iron measured within a 500 um length is always within ±20% of a nominal concentration

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Office Action of JP Appln. No. 2011-260511 dated Jun. 5, 2015.
  • Takashi Saito et al, Development of High Performance Titanium Matrix Composite, R&D Review, vol. 29, No. 3 (1994.9).