Sintered powdered titanium alloy and method of producing the same
Abstract
A sintered titanium alloy is composed of a titanium matrix or titanium alloy matrix and hard particles dispersed in the matrix, the sintered titanium alloy comprises: 4-8 mass % of aluminum (Al); 2-6 mass % of vanadium (V); 0.15-0.8 mass % of oxygen (O); at least one element selected from the group consisting of 0.2-9 mass % of boron (B), 0.5-3 mass % of at least one of molybdenum (Mo), tungsten (W), tantalum (Ta), zirconium (Zr), niobium (Nb), and hafnium (Hf), 0.05-2 mass % of at least one of Ia Group elements, IIa Group elements, and IIIa Group elements, 0.05-0.5 mass % of at least one of halogens; with the balance being titanium (Ti) and inevitable impurities. A method for economically producing a high-density sintered titanium alloy comprises mixing a raw material powder composed of a titanium powder and a powder for solid-solution hardening, rubbing and pressing the titanium powder before, during or after the mixing, so as to cause the raw material powder to have a desired tap density, compacting the mixed powder, and sintering the green compact under no pressure.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 42.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A sintered titanium alloy composed of a titanium matrix or titanium alloy matrix and TiB particles dispersed in said matrix, said sintered titanium alloy comprising: 4-8 mass % of aluminum (Al); 2-6 mass % of vanadium (V); 0.15-0.5% mass % of oxygen (O); and 0.2-1 mass % of boron (B); the balance being titanium and inevitable impurities, and said sintered titanium alloy having a three-phase microstructure of α-phase, β-phase, and TiB particles, wherein α-phase is equiaxed due to a presence of TiB particles so as to enhance a strength of said sintered titanium alloy.
- Claim 2Depends on #1
A sintered titanium alloy as defined in claim 1, which further comprises 0.5-3 mass % of at least one of molybdenum (Mo), tungsten (W), tantalum (Ta), zirconium (Zr), niobium (Nb), and hafnium (Hf), wherein α-phase is equiaxed due to a presence of TiB par
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 42 total)
References Cited — Backward Prior Art (19)
Non-Patent Literature (5)
- F. H. Froes and D. Eylon, "Production Of Titanium Powder", Metals Handbook Ninth Edition, 1982, vol. 7, pp. 164-168.
- F. H. Froes and D. Eylon, Production Of Titanium Powder , Metals Handbook Ninth Edition, 1982, vol. 7, pp. 164 168.
- Journal of Metals, vol. 38, No. 8, Aug. 1986, pp. 36 39, S. Abkowitz, et al., Superior Fatigue Properties For Blended Elemental P/M Ti 6AI 4V .
- Journal of Metals, vol. 38, No. 8, Aug. 1986, pp. 36-39, S. Abkowitz, et al., "Superior Fatigue Properties For Blended Elemental P/M Ti-6AI-4V".