A steel composition and method from making a dual phase steel therefrom. The dual phase steel may have carbon of about 0.05% by weight to about 0.12 wt %; niobium of about 0.005 wt % to about 0.03 wt %; titanium of about 0.005 wt % to about 0.02 wt %; nitrogen of about 0.001 wt % to about 0.01 wt %; silicon of about 0.01 wt % to about 0.5 wt %; manganese of about 0.5 wt % to about 2.0 wt %; and a total of molybdenum, chromium, vanadium and copper less than about 0.15 wt %. The steel may have a first phase consisting of ferrite and a second phase having one or more of carbide, pearlite, martensite, lower bainite, granular bainite, upper bainite, and degenerate upper bainite. A solute carbon content in the first phase may be about 0.01 wt % or less.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for preparing a dual phase steel, comprising: heating a steel slab to a reheating temperature from about 1,000° C. to about 1,250° C., wherein the heating of the steel slab at the reheating temperature provides a steel slab consisting essentially of an austenite phase; reducing the steel slab to form a plate in at least one hot rolling pass at a first temperature, wherein the first temperature is sufficient to recrystallize the austenite phase; reducing the plate in at least one hot rolling pass at a second temperature, wherein the second temperature is from about 700° C. to about 800

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (25)

PatentTitleYearCitations
WO 9,617,965 A1Method of making dual phase steel plate—6
WO 9,617,966 A1Dual-phase steel and method thereof—7
WO 9,617,964 A1Ultra-high strength steels and method thereof—8
US 5,531,842 AMethod of preparing a high strength dual phase steel plate with superior toughness and weldability (LAW219)199655
US 5,545,269 AMethod for producing ultra high strength, secondary hardening steels with superior toughness and weldability199697
US 5,545,270 AMethod of producing high strength dual phase steel plate with superior toughness and weldability199664
US 5,653,826 AHigh strength dual phase steel plate with superior toughness and weldability199750
JP H1017982 AHigh tensile strength steel material with low yield ratio for construction use, excellent in fracture resistance, and its production—36
WO 9,838,345 A1High-tensile-strength steel and method of manufacturing the same—37
JP H10259448 AHigh strength steel sheet excellent in static absorbed energy and impact resistance and its production—21
WO 9,902,747 A1Ultra high strength, secondary hardening steels with superior toughness and weldability—5
US 5,900,075 AUltra high strength, secondary hardening steels with superior toughness and weldability199948
US 6,149,969 AOn-site pipe coating process200013
US 6,565,678 B2Weld metals with superior low temperature toughness for joining high strength, low alloy steels200332
EP 1,325,967 A1High strength steel pipe having strength higher than that of api x65 grade—19
KR 20030081050 AHigh-strength steel sheet and high-strength steel pipe excellent in deformability and method for producing the same—19
US 6,648,209 B2Process for producing welded steel pipes with a high degree of strength, ductility and deformability20039
KR 20040005675 ASteel tube with low yield ratio—3
US 2004050445 A1Steel pipe having low yield ratio—10
US 2004144454 A1Steel plate having superior toughness in weld heat-affected zone and method for manufacturing the same, and welded structure made therefrom—12
US 2006201592 A1High-strength steel pipe of API X65 grade or higher and manufacturing method therefor—23
US 2007193666 A1High Strength Dual Phase Steel With Low Yield Ratio, High Toughness and Superior Weldability—28
WO 2008/045631 A2Low yield ratio dual phase steel linepipe with superior strain aging resistance—6
WO 2008/045631 A3Low yield ratio dual phase steel linepipe with superior strain aging resistance—1
US 8,070,887 B2High-strength steel sheet and high-strength steel pipe excellent in deformability and method for producing the same20118

Non-Patent Literature (5)

  • Atkins et al., “Atlas of Continuous Cooling Transformation Diagrams for Engineering Steels” American Society for Metals, 1980 (pp. 10-16, 153).
  • International Preliminary Report on Patentability, dated Apr. 23, 2009.
  • Office Action in Japanese Patent Application No. 2009-531512 dated Jan. 15, 2013.
  • Office Action in U.S. Appl. No. 12/418,767, dated Oct. 31, 2011.
  • Office Action issued in related Korean Patent Application No. 2009-7008671, dated Apr. 4, 2014, 9 pages.