Patents
US 6,648,209 B2#11455492 Most CitedExpiredUnited States (USPTO)Utility

Process for producing welded steel pipes with a high degree of strength, ductility and deformability

9Forward Citations (#11455492 Global)
0.4/yrCitation Velocity (#20790325 Global)
2.28Citation PageRank (#11789008 Global)
18Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

In a process for producing welded steel pipes, a pipe is molded cold from a TM-rolled sheet, welded together and sized to the desired diameter, whereby the sheet includes steel with (in wt. %) 0.02 to 0.20% carbon, 0.05 to 0.50% silicon, 0.50 to 2.50% manganese, 0.003 to 0.06% aluminum, the remainder being iron with potentially other production-related impurities. After welding and sizing, the pipe is subjected to a heat treatment process at a temperature of 100-300° C. and for a holding time that is suited to the thickness of the pipe wall, with subsequent cooling with air or by forced cooling. The resulting pipe is resistant to aging and has sufficiently integral deformation reserve against fracturing with the same high degree of strength, without exceeding the upper limit for the ratio of yield strength to tensile stress according to the current industry standards for conventional steels.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing welded steel pipes by the UOE-process, comprising the steps of: providing a steel sheet having a composition by wt. % of 0.02 to 0.20% carbon, 0.05 to 0.50% silicon, 0.50 to 2.50% manganese, and 0.003 to 0.06% aluminum, up to 0.02% phosphorus, up to 0.06% titanium, up to 0.20% chromium, up to 0.50% molybdenum, up to 0.30% nickel, up to 0.10% niobium, up to 0.08% vanadium, up to 0.50% copper, up to 0.030% nitrogen, and up to 0.005% boron, the remainder being iron containing production-related impurities; cold-forming, welding and sizing the sheet to a desired diameter to

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (18)

PatentTitleYearCitations
DE 948,604 CHerstellung von verstaerkten Rohrleitungen oder Behaeltern19562
US 4,001,054 AProcess for making metal pipe197737
US 4,160,543 AHeat treatment of welds197917
JP S5735625 AManufacture of high tensile steel pipe with superior toughness at low temperature—6
JP S589926 AProduction of api standard class x80 steel pipe of superior low temperature toughness—10
LU 86,158 A1Procede pour la fabrication en continu de tubes metalliques soudes—2
US 4,945,743 AApparatus for manufacturing electric welded pipes under hot conditions19905
US 4,975,128 AMethod for heat-treating straight bead welded pipes199029
US 5,005,395 AMethod of manufacturing electric welded pipes under hot conditions19918
EP 0,494,448 A1Method for manufacturing electric-resistance-welded steel pipe with high strength—6
JP H06212257 AProduction of steel and steel pipe excellent in corrosion resistance and workability—1
WO 9,600,305 A1Method of increasing the yield strength of cold formed steel sections—2
DE 19,608,387 A1Colouring surface of a steel object—4
DE 19,522,790 A1Verfahren zur Herstellung von Rohren nach dem UOE-Verfahren—2
US 6,331,216 B1Steel pipe having high ductility and high strength and process for production thereof200125
US 2002117538 A1Process for producing welded steel pipes with a high degree of strength, ductility and deformability—5
US 2002117239 A1Ferritic stainless steel sheet having good workability and manufacturing method thereof—12
US 2002136661 A1Ferritic stainless steel sheet with excellent workability and method for making the same—12