The invention provides an ethylene-based polymer comprising the following properties: a) weight fraction (w) of molecular weight above 5*10 6 g/mol, w>A−B*I2, where A=0.4 wt %, and B is 0.02 wt %/(dg/min), and w<C−B*I 2 %, where C=0.9 wt %; and b) G′>D−E*log(I2), where D=162 Pa and E=52 Pa/log(dg/min).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 14.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An ethylene-based polymer comprising the following properties: a) weight fraction, as a percentage (w) of molecular weight above 5*10 6 g/mol, w>A−B*I2, where A=0.4 wt %, and B is 0.02 wt %/(dg/min), and w<C−B*I 2 %, where C=0.9 wt %; b) G′ (at G″ equal to 500 Pa, 170° C.)>D−E*log(I2), where D=162 Pa and E=52 Pa/log(dg/min), c) a Mw(abs)/Mn(abs) from 17.0 to 24.0; and d) n-hexane extractables <X wt %+Y*log(I 2 ), where X=2.3 wt % and Y=1.66 wt %/log(dg/min).
- Claim 2Depends on #1
The ethylene-based polymer of claim 1 , wherein the polymer has a melt index (I 2 ) from 0.3 to 16 dg/min.
- Claim 3Depends on #1
The polymer of claim 1 , in which the polymer has a n-hexane extractable level less than or equal to 3.5 wt %.