Preparation of polyethylene
Abstract
Ethylene homopolymers and copolymers are prepared in a tube reactor at from 160° C. to 350° C. and pressures in the range from 500 to 5000 bar, with or without use of molar mass regulators, using a peroxide mixture comprising from 1 to 95 mol %, based on the total amount of the peroxide mixture, of at least one cyclic peroxide of the formula I, where the radicals R are identical or different and are selected from among alkyl groups and aryl groups, as polymerization initiator.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 21.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for preparing ethylene homopolymers or copolymers in a tube reactor at from 160° C. to 350° C. and pressures in the range of 500 to 5000 bar, with or without use of molar mass regulators, wherein a peroxide mixture comprising A) from 1 to 50 mol % of one or more trimeric ketone peroxides of the formula I as peroxides decomposing at high temperature where the radicals R are identical or different and are selected from among alkyl groups or aryl groups, and B) from 50 to 99 mol % of one or more conventional polymerization initiators, the mol % being based on the total weight of the per
- Claim 2Depends on #1
A process as claimed in claim 1 , wherein the radicals R are selected from among linear C 1 -C 8 -alkyl groups.
- Claim 3Depends on #1
A process as claimed in claim 1 , wherein all the radi
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗