Patents
US 9,754,824 B2#45364992 Most CitedActiveUnited States (USPTO)Utility

Tungsten films having low fluorine content

2Forward Citations (#45364992 Global)
0.2/yrCitation Velocity (#31911722 Global)
0.86Citation PageRank (#49894458 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Aspects of the methods and apparatus described herein relate to deposition of tungsten nucleation layers and other tungsten-containing films. Various embodiments of the methods involve exposing a substrate to alternating pulses of a tungsten precursor and a reducing agent at low chamber pressure to thereby deposit a tungsten-containing layer on the surface of the substrate. According to various embodiments, chamber pressure may be maintained at or below 10 Torr. In some embodiments, chamber pressure may be maintained at or below 7 Torr, or even lower, such as at or below 5 Torr. The methods may be implemented with a fluorine-containing tungsten precursor, but result in very low or undetectable amounts of fluorine in the deposited layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method comprising: exposing a substrate to alternating pulses of a fluorine-containing tungsten precursor and a reducing agent to thereby deposit a tungsten-containing film on the substrate, wherein a chamber pressure of a chamber housing the substrate during the fluorine-containing tungsten precursor pulses is less than 10 Torr, and wherein the total fluorine concentration in the tungsten-containing film is less than 10 18 atoms/cm 3 .

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the chamber pressure is less than 7 Torr.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the chamber pressure is less than 5 Torr.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
JP S5629648 AHigh hardness sintered body—23
US 4,746,375 AActivation of refractory metal surfaces for electroless plating198880
US 4,804,560 AMethod of selectively depositing tungsten upon a semiconductor substrate1989123
US 4,874,719 AMethod for manufacturing an electrical connection between conductor levels198995
JP H02187031 ASemiconductor device—41
US 4,962,063 AMultistep planarized chemical vapor deposition process with the use of low melting inorganic material for flowing while depositing1990114
US 5,028,565 AProcess for CVD deposition of tungsten layer on semiconductor wafer1991173
EP 0,437,110 A2Tungsten deposition process for low contact resistivity to silicon—24
JP H04142061 AFormation of tungsten plug—44
US 5,227,329 AMethod of manufacturing semiconductor device1993172
JP H05226280 AManufacture of semiconductor device—49
US 5,250,329 AMethod of depositing conductive lines on a dielectric199375
US 5,250,467 AMethod for forming low resistance and low defect density tungsten contacts to silicon semiconductor wafer1993116
US 5,308,655 AProcessing for forming low resistivity titanium nitride films199466
US 5,326,723 AMethod for improving stability of tungsten chemical vapor deposition1994145
US 5,370,739 ARotating susceptor semiconductor wafer processing cluster tool module useful for tungsten CVD1994149
US 5,391,394 ATungsten deposition process for low contact resistivity to silicon1995112
US 5,407,698 ADeposition of tungsten199597
JP H07147321 AManufacture of semiconductor device—44
JP H07226393 AMethod and apparatus for dry-etching—53
JP H08115984 ASemiconductor device and its manufacture—28
US 5,567,583 AMethods for reducing non-specific priming in DNA detection1996122
JP H0922896 AMethod of selective forming of metal film—47
JP H0927596 AManufacture of semiconductor device—27
US 5,633,200 AProcess for manufacturing a large grain tungsten nitride film and process for manufacturing a lightly nitrided titanium salicide diffusion barrier with a large grain tungsten nitride cover layer1997135
EP 0,310,461 B1Pressure-generating device for automotive vehicle breaking circuits19920
US 5,661,080 AMethod for fabricating tungsten plug199792
US 5,726,096 AMethod for forming a tungsten silicide layer in a semiconductor device199893