Deposition of tungsten

97Forward Citations (#251460 Global)
3.1/yrCitation Velocity (#810329 Global)
20.82Citation PageRank (#312289 Global)
10Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method is provided for low pressure chemical deposition of tungsten and tungsten metallization for defining interconnects for an integrated circuit. A surface layer of tungsten is provided which has a low film stress and a smooth surface characterized by a low diffuse reflectivity and high specular reflectivity, to facilitate photo-lithography. Tungsten is deposited by reduction of WF 6 with H 2 and SiH 4 in nitrogen. Control of the gas flow rates, pressure, temperature and H 2 /WF 6 ratio in the reactive gas mixture provides for tailoring of the structure and characteristics of a deposited tungsten layer to provide high step coverage or a smooth surface for forming an overlying layer of tungsten which may be patterned photo-lithographically for defining interconnect. In order to provide metallization providing both good step coverage in via and contact holes and smooth surface for deposition of surface metallization, a two-stage tungsten deposition is provided.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 97.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for chemical vapour deposition of tungsten for an integrated circuit, comprising: exposing a substrate to a mixture of reactive gases consisting of WF 6 , H 2 and a carrier gas consisting essentially of nitrogen, maintaining a pressure between 1 and 9 Torr, a deposition temperature between 430° C. and 500° C., and controlling the relative flow rates of H 2 and WF 6 to provide a H 2 /WF 6 flow rate ratio of between 5 and 30, the mixture of gases thereby depositing on the substrate a layer of tungsten having a smooth surface.

  2. Claim 2Depends on #1

    A method according to claim 1 wherein the flow rate of WF 6 is maintained in the range 10 to 40 sccm and the reactive gas mixture includes up to 15 sccm of SiH 4 .

  3. Claim 3Depends on #1

    A method according to claim 1 wherein a first thickness of tungsten is deposited while maintaining a H 2

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • R. W. Haskell & J. G. Byrne "Studies in Chemicial Vapour Deposition". Treatise Mater. Sci. Techno 1972, vol. 1, pp. 293-340; ed. H. Herbert (Academic Press N.Y.) month not known.
  • R. W. Haskell & J. G. Byrne Studies in Chemicial Vapour Deposition . Treatise Mater. Sci. Techno 1972, vol. 1, pp. 293 340; ed. H. Herbert (Academic Press N.Y.) month not known.
  • Riley et al., "Integrated Chemical Vapor Deposition and Plasma Etchback of Tungsten", J. Electrochem. Soc., v. 138, No. 10, pp. 3008-3013 (Oct. 1991).
  • Riley et al., Chemical Abstracts, 115:245594t (1991). month not known.
  • Riley et al., Integrated Chemical Vapor Deposition and Plasma Etchback of Tungsten , J. Electrochem. Soc., v. 138, No. 10, pp. 3008 3013 (Oct. 1991).