Sealing method for silicon carbide parts used at high temperatures

0Forward Citations (#119683682 Global)
0.0/yrCitation Velocity (#119683682 Global)
0.56Citation PageRank (#119683682 Global)
23Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present disclosure describes silicon carbide articles useful at high temperatures, and the method of making them. The method includes: providing a plurality of silicon carbide parts; providing a mullite gasket; placing the gasket between the ends of the parts to be joined to thereby form an assembly; applying a load in the range of 15-25 pounds per square inch to the parts' ends distal from the gasket to thereby press the gasket; heating the assembly in a muffle furnace under load to a temperature in the range of 1450° C. to 1550° C.; increasing the load on the to range of 30-50 pounds per square inch and holding the assembly at the temperature for a time in the range of 2-5 days to adhere the mullite gasket to the ends of the silicon carbide parts.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for joining and sealing at least two silicon carbide parts, the method comprising: placing a solid fully dense mullite gasket between and in contact with ends of at least two silicon carbide parts to be joined to thereby form an assembly, wherein said solid fully dense mullite gasket comprises a combined Al 2 O 3 plus SiO 2 content of at least 97 wt. % and 3 wt. % or less of oxide modifiers; and heating the assembly so that the solid fully dense mullite gasket forms a bond between the ends of the at least two silicon carbide parts, wherein the bond is chemically and physically stabl

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the act of heating the assembly comprises applying a load in the range of 15-25 pounds per square inch to ends of the at least two silicon carbide parts tha

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (23)

PatentTitleYearCitations
US 3,932,162 AMethod of making glass optical waveguide197698
US 4,070,197 AGas tight silicon carbide body197820
GB 2,072,313 AMuffle furnace—6
US 4,499,360 AMethod of brazing silicon carbide parts using Si-Co solder198517
US 4,640,899 AMullite matrix composite198732
US 4,762,269 AMethod of joining molded silicon carbide parts198840
US 5,183,490 AOptical fiber soot synthesis apparatus199317
US 5,407,504 AMethod for joining ceramic to ceramic or to carbon199522
JP H09188580 AMullite mortar and correction of surface shape of silicon carbide shelf board using the same—4
US 6,467,310 B2Method for producing optical fiber base material ingot by grinding while core portion central axis is brought into line with rotational axis of grinding machine20024
US 2003003329 A1Coated article and method of making—19
US 2003138596 A1Honeycomb filter and method for manufacturing the same—36
US 2007166570 A1Method of forming a ceramic to ceramic joint—10
US 7,462,255 B2Method for producing by laser gastight and high-temperature resistant connections of shaped parts made of a non-oxidic ceramic20082
US 2008304959 A1Joint Between a Metal Part and a Ceramic Part Based Sic and/or C—18
US 2010055498 A1Process for the Moderately Refractory Assembling of Articles Made of SiC-Based Materials by Non-Reactive Brazing in an Oxidizing Atmosphere, Brazing Compositions, and Joint and Assembly Obtained by this Process—6
US 7,695,580 B2Method of forming a ceramic to ceramic joint20109
WO 2010/049909 A1Body assembled with a macroporous hardened cement—5
US 2010255289 A1Aluminosilicate-Based Oxide Composite Coating and Bond Coat for Silicon-Based Ceramic Substrates—33
JP 2012051807 AArylimidazole compound—8
WO 2012/102378 A1Silicon carbide assembly, heat transfer tube comprising same, and heat exchanger provided with said heat transfer tube—4
US 2012304701 A1Manufacturing method of optical fiber base material possessing low refractive index portion distantly-positioned from core—8
US 2013266363 A1High durability joints between ceramic articles, and methods of making and using same—12

Non-Patent Literature (5)

  • Briot et al. “WO 2010/049909, machine translation”, published May 6, 2010.
  • DATABASE WPI Week 198328, 7 June 1983 Derwent World Patents Index; XP002726722, "Joining silicon carbide ceramic articles - by interposing mixt. of silicon carbide and carbon between silicon carbide articles, etc."
  • Database WPI, Thomson Scientific, London, GB; AN 1983-709021, XP002726722, & JP S58 95667 A (Toyota Jidosha KK), Jun. 7, 1983, Abstract.
  • International Search Report and Written Opinion PCT/US2014/035644 Dated Jul. 23, 2014.
  • Ishiguro et al. “JP 09-188580, machine translation”, published Jul. 22, 1997.