Abstract

Method for producing by laser gastight and high-temperature resistant connections of shaped parts made of non-oxidic ceramic. The invention relates to the fields of ceramics and laser technology and relates to a method with which, e.g., low-melting-point or radioactive materials can be enclosed inside a container made of ceramic. The object of the invention is to produce a durable, gastight and high-temperature resistant connection between components made of non-oxidic ceramic. Shaped parts made of the ceramic are provided on the surfaces to be joined with a solder of 80-30% by weight yttrium oxide and/or 55-15% by weight zirconium oxide, 20-70% by weight aluminum oxide, 0-50% by weight silicon dioxide and 0-10% by weight silicon, and subsequently the temperature at the joint area is increased above the melting temperature of the solder by means of a laser without the presence of a protective gas atmosphere or a vacuum.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 31 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing gastight and high-temperature resistant connection of shaped parts, the parts made of a non-oxidic ceramic, comprising: providing solder at a joint area at surfaces of the shaped parts to be joined, the solder comprising at least one of 80-30% by weight yttrium oxide and 55-15% by weight zirconium oxide, 5-70% by weight aluminum oxide, 0-50% by weight silicon dioxide and 0-10% by weight silicon, and having a melting temperature; and subsequently raising a temperature at the joint area above the melting temperature of the solder by a laser, without presence of a protectiv

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (31)

PatentTitleYearCitations
US 3,876,408 AConnections between glass and silicon or silicon carbide19756
DE 2,627,993 A1Verfahren zur herstellung von siliciumcarbid-hohlkoerpern—4
US 4,070,197 AGas tight silicon carbide body197820
JP S5832593 AWelding method—6
JP S5836985 AJoint method—5
JP S6071913 AElectromagnetic flowmeter—2
DE 3,539,651 A1Application of a wear-resistant layer to a furnace lining—6
US 4,729,973 AProcess for producing ceramic composites from microcomposite particles having dispersed fibrous microstructures and the product thereof198812
US 4,763,828 AMethod for bonding ceramics and metals1988114
JP S63225584 ALaser-activated soldering process for ceramics—3
US 4,798,991 ASurface-gap spark plug for internal combustion engines198930
US 5,059,095 ATurbine rotor blade tip coated with alumina-zirconia ceramic1991162
US 5,098,494 ABonding of ceramic parts199217
US 5,116,786 ALow temperature sealing glass composition199220
DE 4,116,865 A1Porous composite bodies prodn. - by coating ceramic particles with silicon carbide and joining together with silicon solder—1
JP H05261586 ACream solder—9
JP H07187836 AMethod for joining si-containing ceramics with laser light—8
US 5,451,279 AMethod for joining ceramic sintered bodies199535
US 5,503,703 ALaser bonding process199632
US 5,512,327 AProcedure for producing a highly porous catalyst layer consisting of a palladium or platinum alloy199624
DE 19,540,900 A1Joining moulded silicon carbide bodies to form gas-tight seal—2
US 5,874,175 ACeramic composite199978
US 5,893,328 AMethod of controlled laser imaging of zirconia-alumina composite ceramic lithographic printing member to provide localized melting in exposed areas199928
US 5,912,914 AInsulated laser tube structure and method of making same19999
JP 2001354448 ASealing glass for joining stem of electron gun to cathode- ray tube, stem of electron gun and cathode-ray tube—4
US 6,448,777 B1Hermetically-sealed miniaturized discharge ionization detector200230
US 6,543,134 B2Method for reconditioning blades200322
US 6,586,704 B1Joining of materials using laser heating200319

Non-Patent Literature (5)

  • A. Hesse et al., Keramische Zeitschrift, vol. 46, No. 3, 1994, pp. 147-150.
  • A.-M. Reinecke et al., Lasermagazin, vol. 5, 2002, pp. 18.
  • B. Wielage et al., VDI-Berichte, vol. 883, pp. 117-136, VDI-Verlag, Dusseldorf, 1991.
  • Database WPI, Section CH, Week 198315, Derwent Publications Ltd., London, GB, Class 102, AN 1983-3552K.
  • Database WPI, Section Ch, Week 198843, Derwent Publications Ltd., London, GB; Class L02, AN 1988-304859.