Patents
US 9,701,561 B2#45475571 Most CitedActiveUnited States (USPTO)Utility

High purity synthetic silica and items such as semiconductor jigs manufactured therefrom

2Forward Citations (#45475571 Global)
0.2/yrCitation Velocity (#31918145 Global)
0.86Citation PageRank (#50252992 Global)
31Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Hollow ingots of transparent synthetic vitreous silica glass of external diameter greater than 400 mm and internal diameter greater than 300 mm are disclosed. The ingots are substantially free from bubbles or inclusions greater than 100 μm in diameter, have no more than 100 ppB of any individual metallic impurity, and have chlorine concentration less than 5 ppM. Also disclosed are methods for producing such ingots, in which a porous soot body of density greater than 0.4 g/cm 3 is deposited on an oxidation resistant mandrel. The soot body is dehydrated on a mandrel comprising graphite, carbon fiber reinforced carbon, silicon carbide, silicon impregnated silicon carbide, silicon carbide-coated graphite or vitreous silica, either under vacuum or in the presence of a reducing gas, and then sintered to transparent pore-free glass under vacuum or in an atmosphere of helium.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 31 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the manufacture of an annular semiconductor jig of transparent synthetic vitreous silica suitable for use in a plasma etching environment, said jig having an external diameter greater than 400 mm and an internal diameter greater than 300 mm, wherein said jig is substantially free from bubbles or inclusions greater than 100 μm in diameter; has no more than 100 ppB of any individual metallic impurity; and has chlorine concentration less than 380 ppB, the process comprising the steps of: depositing a porous soot body of density greater than 0.4 g/cm 3 on an oxidation resistant mand

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (31)

PatentTitleYearCitations
US 3,109,121 AArc welding control system19633
US 4,047,966 AMethod of enhancing the refractoriness of high purity fused silica197736
US 4,191,545 AOptical fiber fabrication process198012
EP 0,163,752 A1A method for the preparation of a synthetic quartz glass tube—26
US 5,180,410 AMethod of making polarization retaining fiber199324
US 5,262,365 AQuartz glass doped with rare earth element and production thereof199360
JP H09227143 AOpaque quartz glass and its production—2
WO 0,208,129 A1Method for the vitrification of a porous soot body—7
US 2002037797 A1Fluorine-containing glass—5
US 6,376,401 B1Ultraviolet ray-transparent optical glass material and method of producing same200232
US 2004118155 A1Method of making ultra-dry, Cl-free and F-doped high purity fused silica—34
US 6,887,576 B2Quartz glass body having improved resistance against plasma corrosion, and method for production thereof200514
US 2005187092 A1Synthetic silica glass optical material having high resistance to laser induced damage—20
US 2006059948 A1Method for producing synthetic quartz glass and synthetic quartz glass article—21
US 7,084,084 B2Highly durable silica glass, process for producing same, member comprised thereof, and apparatus provided therewith200613
US 7,082,789 B2Silica glass member for semiconductor and production method thereof20064
US 7,275,397 B2Method of molding a silica article20074
WO 2007/135166 A1Method for producing a semifinished product from synthetic quartz glass—3
US 2008053151 A1Mixed powder and a method for producing quartz glass using the powder—5
US 2008066497 A1Holder Made From Quartz Glass for the Processing of Semiconductor Wafers and Method for Production of the Holder—20
US 7,365,037 B2Quartz glass having excellent resistance against plasma corrosion and method for producing the same200813
EP 2,070,883 A1Fused quartz glass and process for producing the same—16
US 2009163344 A1Component of Quartz Glass for Use in Semiconductor Manufacture and Method for Producing the Same—9
EP 2,088,129 A2Halide free fused silica glasses having low OH, OD concentrations and their manufacturing method—3
US 7,661,277 B2Quartz glass having excellent resistance against plasma corrosion and method for producing the same20108
US 2011072852 A1Method for the production of a cylinder made from quartz glass using a retaining device, and retaining device—8
US 8,230,701 B2Method for forming fused silica glass using multiple burners201210
US 2013045854 A1Manufacture of synthetic silica glass—7

Non-Patent Literature (5)

  • "Fused Quartz Properties & Usage Guide", http://www.quartz.com/gedata.html, Feb. 1996.
  • International Search Report and Written Opinion dated Oct. 31, 2011 issued in International Patent Application No. PCT/EP2011/061683.
  • Office action dated Jun. 9, 2014 issued in co-pending U.S. Appl. No. 13/581,974.
  • Printed copy of http://www.schunkgraphite.com/en/sgt/Coating-Service/schunk01.c.39140.en, accessed Mar. 31, 2015.
  • Schmet et al, High-temperature oxidation behavior of carbon materials in air, Carbon, 31(1):1-6 (1993).