US 7,082,789 B2#22959666 Most CitedExpiredUnited States (USPTO)Utility

Silica glass member for semiconductor and production method thereof

4Forward Citations (#22959666 Global)
0.2/yrCitation Velocity (#32617086 Global)
2.01Citation PageRank (#14402329 Global)
7Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A silica glass member for semiconductor in which each concentration of Fe, Cu, Cr and Ni is 5 ppb or less and the concentration of an OH group is 30 ppm or less and which has a viscosity of 10 13.0 poise or more at 1200° C. is provided as a silica glass member for semiconductor having high heat-resistance and higher purity.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 4.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a silica glass member for use in production of a semiconductor comprising heat-treating a silica glass base material in which each concentration of Fe, Cu, Cr and Ni is 100 ppb or less and the concentration of an OH group is 50 ppm or less and which has a viscosity of 10 13.0 poise or more at 1200° C., at a temperature of 1100° C. or more in a non-acidic atmosphere and then etching the entire surface by using hydrofluoric acid.

  2. Claim 2Independent Claim

    A method of producing a silica glass member for use in production of a semiconductor comprising etching the entire surface of a silica glass base material in which each concentration of Fe, Cu, Cr and Ni is 100 ppb or less and the concentration of an OH group is 50 ppm or less and which has a viscosity of 10 13.0 poise or more at 1200° C., by using hydrofluoric acid and then heat-treating the silica glass material at a t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗