Patents
US 9,640,320 B2#101206767 Most CitedActiveUnited States (USPTO)Utility

Method of producing grain-oriented electrical steel sheet

0Forward Citations (#101206767 Global)
0.0/yrCitation Velocity (#101206767 Global)
0.56Citation PageRank (#101206767 Global)
26Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

In a method of producing a grain-oriented electrical steel sheet by subjecting a coil for grain-oriented electrical steel sheet after cold rolling to a primary recrystallization annealing, applying an annealing separator thereon, and conducting final annealing, rapid heating is conducted at a rate of not less than 80° C./sec from 500° C. to 700° C. in the course of heating for the primary recrystallization annealing, and a temperature keeping treatment is conducted for 2 to 100 hours from 700° C. to 1000° C. in the course of heating for the final annealing, and further, the final annealing is preferably conducted by laying a thermal insulation material on an upper surface of a coil supporting stand in an annealing furnace used for the final annealing concentrically from the outer periphery of the coil supporting stand and over an area of not less than 20% of the radius of the coil supporting stand.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 0.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a grain-oriented electrical steel sheet having forsterite film by subjecting a coil for grain-oriented electrical steel sheet after cold rolling to a primary recrystallization annealing, applying an annealing separation agent composed mainly of MgO thereon, and conducting final annealing, wherein for the primary recrystallization annealing rapid heating is conducted at a rate of not less than 80° C./sec from 500° C. to 700° C., and for the final annealing a temperature keeping treatment is conducted for 2 to 100 hours by maintaining a constant keeping temperature from 700

  2. Claim 2Independent Claim

    The method of producing a grain-oriented electrical steel s

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (26)

PatentTitleYearCitations
JP S5943818 AProduction of unidirectional silicon steel sheet having excellent magnetic characteristic—3
US 4,504,957 AHigh temperature box annealing furnace198520
US 4,898,626 AUltra-rapid heat treatment of grain oriented electrical steel199037
JP H0551643 AFinish annealing method for grain-oriented magnetic steel sheet—6
JP H06128646 AProduction of grain oriented silicon steel sheet reduced in iron loss and having high magnetic flux density—14
US 5,833,768 AGrain-oriented electrical steel sheet with very low core loss and method of producing the same199816
US 2002038678 A1Method to produce grain-oriented electrical steel sheet having high magnetic flux density—14
CN 1,708,594 AMethod for producing grain-oriented electrical steel sheet, and grain-oriented electrical steel sheet—13
JP 2006257486 AMethod for annealing grain oriented electrical steel sheet, and inner cover for batch annealing of grain oriented electrical steel sheet—12
JP 2006274343 AHolder in final finish annealing for grain-oriented electromagnetic steel sheet—6
US 7,291,230 B2Grain-oriented electrical steel sheet extremely excellent in film adhesiveness and method for producing the same20073
US 7,465,361 B2Method for producing grain oriented magnetic steel sheet and grain oriented magnetic steel sheet20084
US 2010005481 A1Method of Maintaining Applications in a Computing Device—31
US 2010055481 A1Grain-oriented electrical steel sheet excellent in coating adhesion and method of producing the same—35
CN 101,778,964 AInsulating coating treatment liquid for grain oriented electromagnetic steel sheet and process for manufacturing grain oriented electromagnetic steel sheet with insulating coating—5
JP 2010236013 AMethod for producing grain-oriented magnetic steel sheet—33
JP 2011006738 AMethod for winding nitridation-type grain-oriented electromagnetic steel sheet which has been nitrided into coil—8
US 2011067786 A1Treatment solution for insulation coating for grain oriented electrical steel sheet and method for producing grain oriented electrical steel sheet having insulation coating—14
US 2011155285 A1Manufacturing method of grain-oriented electrical steel sheet—11
JP 2011174138 AMethod for manufacturing grain-oriented electromagnetic steel sheet—26
KR 20120074030 AMethod for manufacturing grain-oriented electrical steel sheets having excellent magnetic properties—2
JP 2012126989 AMethod for producing directional electromagnetic steel sheet—12
US 8,771,795 B2Treatment solution for insulation coating for grain-oriented electrical steel sheets and method for producing grain-oriented electrical steel sheet having insulation coating20144
US 2014251514 A1Grain-oriented electrical steel sheet and method of producing the same (as amended)—9
US 2014338794 A1Method of producing grain-oriented electrical steel sheet having excellent iron loss properties—14
US 2015007908 A1Method for producing oriented electromagnetic steel sheet—13

Non-Patent Literature (5)

  • European Office Action for Application No. 12824506.5, dated Jun. 14, 2016.
  • European Search Report mailed Jun. 5, 2015 for European Application No. 12824506.5.
  • Final Office Action dated Nov. 20, 2015 for U.S. Appl. No. 14/431,577.
  • Final Office Action mailed Sep. 8, 2016 for U.S. Appl. No. 14/431,577, 8 pages.
  • International Preliminary Report on Patentability and Written Opinion dated Feb. 18, 2014, application No. PCT/JP2012/070238.