Abstract

In a method for manufacturing a grain-oriented electrical steel sheet using steel containing less than 100 ppm of Al and 50 ppm or less each of N, S, and Se as a starting material, purification annealing is performed at 1050° C. or more, the partial pressure of hydrogen in the atmosphere being adjusted to 0.4 atm or less in a temperature range above 1170° C. for a purification annealing conducted at a temperature above 1170° C., or 0.8 atm or less in a temperature range of 1050° C. or more for a purification annealing conducted at a temperature of 1170° C. or less, to prevent deterioration of the bend properties due to the impurities.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a grain-oriented electrical steel sheet, comprising the steps of: rolling a steel slab containing 0.08 mass percent or less of carbon, 2.0-8.0 mass percent of Si, and 0.005-3.0 mass percent of Mn into a cold-rolled steel sheet; subsequently performing decarburizing annealing of the cold-rolled steel sheet if desired; subsequently applying an annealing separator to the cold-rolled steel sheet if desired; performing secondary-recrystallization annealing of the cold-rolled steel sheet; and subsequently performing purification annealing of the cold-rolled steel sheet, wh

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Partial Translation of Korean Patent Publication No. 1993-7161.