US 9,604,851 B2#137493869 Most CitedActiveUnited States (USPTO)Utility

Method for producing high silica zeolite using recovered silica filtrate, and high silica zeolite produced according to said method

0Forward Citations (#137493869 Global)
0.0/yrCitation Velocity (#137493869 Global)
0.56Citation PageRank (#137493869 Global)
9Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Provided are a method of manufacturing a high silica zeolite using a recovered silica filtrate, and a high silica zeolite manufactured according to the method. To this end, the present invention provides the method of manufacturing the high silica zeolite using the recovered silica filtrate, including manufacturing a solated agglomerated silica from the silica filtrate including a metal salt (step 1); filtering and washing the solated agglomerated silica of step 1 to manufacture a silica cake from which the metal salt is removed (step 2); peptizing the silica cake to manufacture a silica sol (step 3); and manufacturing the high silica zeolite using the silica sol manufactured in step 3 as a silica source (step 4). Further, the present invention provides a high silica zeolite manufactured from a recovered silica filtrate through the manufacturing method and having a Si/Al mole ratio of 5 or more. According to the present invention, it is possible to provide a process of manufacturing a high silica zeolite, in which economic feasibility, a manufacturing cost, and a manufacturing time of process steps are reduced, by reusing a recovered silica filtrate to manufacture the zeolite.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a high silica zeolite using a recovered silica filtrate, comprising: manufacturing a solated agglomerated silica from a silica filtrate including a metal salt (step 1); filtering and washing the solated agglomerated silica of step 1 to manufacture a silica cake from which the metal salt is removed (step 2); peptizing the silica cake to manufacture a silica sol (step 3); and manufacturing the high silica zeolite using the silica sol manufactured in step 3 as a silica source (step 4).

  2. Claim 2Depends on #1

    The method as set forth in claim 1 , wherein in step 1, the solated agglomerated silica is manufactured by growing the silica filtrate including the metal salt from a nucleus, and performing solation and then agglomeration.

  3. Claim 3Depends on #2

    The method as set forth in claim 2 , wherein the nucleus is ge

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (2)

  • Huihua Pan, et al; "A Green and Efficient Synthesis of ZSM-5 Using NaY as Seed with Mother Liquid Recycling and in the Absence of Organic Template", Ind. Eng. Chem. Res. vol. 49, pp. 7294-7302; Published on Web Jul. 14, 2010.
  • International Search Report mailed Oct. 14, 2013; PCT/KR2013/005900.