Preparation of silica sols
Abstract
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 13.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A METHOD OF PREPARING A SILICA SOL STABLE AT SILICA CONCENTRATIONS UP TO 30% WHICH COMPRISES PREPARING AN ALKALINE SILICA HYDROGEL BY INCOMPLETELY NEUTRALIZING AN ALKALI METAL SILICATE SOLUTION BY COMMINGLING THEREWITH LESS THAN THE STOICHIOMETRIC AMOUNT OF ACID REQUIRED TO NEUTRALIZE THE ALKALI IN THE SILICATE SOLUTION, WASHING SAID HYDROGEL WITH DEIONIZED WATER TO REMOVE SOFUBLE ALKALI METALS SALTS, GRADUALLY RAISING THE TEMPERATURE OF SAID HYDROGEL AT A PH BETWEEN 9 AND 9.5 UNDER NON-EVEPORATIVE CONDITIONS OVER A PERIOD OF ABOUT 6 HOURS TO 95*-100* C. MAINTAING THE HYDROGEL AT SAID TEMPERAT