Method for producing a blank of fluorine-doped and titanium-doped glass having a high silicic-acid content and a blank produced according to the method
Abstract
A method for producing a silica glass blank co-doped with titanium and fluorine for use in EUV lithography includes (a) producing a TiO 2 —SiO 2 soot body by flame hydrolysis of silicon- and titanium-containing precursor substances, (b) fluorinating the TiO 2 —SiO 2 soot body to form a fluorine-doped TiO 2 —SiO 2 soot body, (c) treating the fluorine-doped TiO 2 —SiO 2 soot body in a water vapor-containing atmosphere to form a conditioned soot body, and (d) vitrifying the conditioned soot body to form the blank. The blank has an internal transmission of at least 60% in the wavelength range of 400 to 700 nm at a sample thickness of 10 mm, a mean OH content in the range of 10 to 100 wt. ppm and a mean fluorine content in the range of 2,500 to 10,000 wt. ppm. Titanium is present in the blank in the oxidation forms Ti3 + and Ti 4+ .
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for producing a blank of titanium-doped glass having a high silicic acid content, an internal transmission of at least 60% in a wavelength range of 400 nm to 700 nm at a sample thickness of 10 mm, and a given fluorine content for use in extreme ultraviolet lithography, the titanium being present in oxidation forms Ti 3+ and Ti 4+ , the method comprising the steps of: (a) producing a TiO 2 —SiO 2 soot body by flame hydrolysis of silicon- and titanium-containing precursor substances; (b) fluorinating the TiO 2 —SiO 2 soot body to form a fluorine-doped TiO 2 —SiO 2 soot body; (c) tre
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (17)
Non-Patent Literature (5)
- D.S. Carson et al., "Optical Attenuation in Titania-Silica Glasses," Journal of Non-Crystalline Solids, vol. 11, pp. 368-380 (1973).
- Dodd et al., "Optical Determinations of OH in Fused Silica," Communications, p. 3911 (1966).
- K. Saito et al., "Effects of fluorine on structure, structural relaxation, and absorption edge in silica glass," Journal of Applied Physics, vol. 91, No. 8, pp. 4886-4890 (Apr. 15, 2002).
- Pfleiderer et al., "The UV-induced 210 nm absorption band in fused silica with different thermal history stoichiometry," Journal of Non-Crystalline Solids, vol. 159, pp. 145-153 (1993).
- Schoedel, "Ultra-high accuracy thermal expansion measurements with PTB's precision interferometer," Measurement Science and Technology, vol. 19, pp. 1-11 (2008).