TiO2-containing silica glass
Abstract
The present invention is to provide a TiO 2 —SiO 2 glass having suitable thermal expansion properties as an optical member of an exposure tool for EUVL. The present invention relates to a TiO 2 -containing silica glass having a temperature, at which a coefficient of thermal expansion is 0 ppb/° C., falling within the range of 23±4° C. and a temperature width, in which a coefficient of thermal expansion is 0±5 ppb/° C., of 5° C. or more.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 14.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A TiO 2 -containing silica glass having a temperature, at which a coefficient of thermal expansion is 0 ppb/° C., falling within a range of 23±4° C., a temperature width, in which a coefficient of thermal expansion is 0±5 ppb/° C., of 5° C. or more, and an OH concentration of 100 ppm or more.
- Claim 2Depends on #1
The TiO 2 -containing silica glass according to claim 1 , having a fictive temperature of not higher than 850° C., and a TiO 2 content of from 3 to 9% by mass.
- Claim 3Depends on #1
The TiO 2 -containing silica glass according to claim 1 , wherein the temperature, at which a coefficient of thermal expansion is 0 ppb/° C., is within a range of 22 ±2° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (14 of 14 total)
References Cited — Backward Prior Art (24)
Non-Patent Literature (4)
- U.S. Appl. No. 12/862,174, filed Aug. 24, 2010, Koike, et al.
- U.S. Appl. No. 12/868,900, filed Aug. 26, 2010, Koike, et al.
- U.S. Appl. No. 12/869,035, filed Aug. 26, 2010, Koike, et al.
- U.S. Appl. No. 12/870,156, filed Aug. 27, 2010, Koike, et al.