Patents
US 9,307,639 B2#61056555 Most CitedActiveUnited States (USPTO)Utility

Electro-deposited copper foil, surface-treated copper foil using the electro-deposited copper foil and copper clad laminate using the surface-treated copper foil, and a method for manufacturing the electro-deposited copper foil

1Forward Citations (#61056555 Global)
0.1/yrCitation Velocity (#46365162 Global)
0.75Citation PageRank (#61056555 Global)
22Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Present invention provides an electro-deposited copper foil having the equivalent low-profile surface as in a conventional low-profile electro-deposited copper foil and extremely large mechanical strength and a method for manufacturing the same. The electro-deposited copper foil is formed by depositing fine copper crystal grains having a small deviation of grain-diameter. The electro-deposited copper foil has a low-profile and glossy surface and has extremely large mechanical strength expressed by a tensile strength as received of 70 kgf/mm 2 to 100 kgf/mm 2 and has a tensile strength after heating (180° C. for 60 minutes) corresponding to 85% or more of the tensile strength as received. The electro-deposited copper foil is manufactured by electrolysis using a sulfuric acid base copper electrolytic solution containing a compound composed of a benzene ring having a sulfo group bonded thereto, a sulfonate of an active sulfur compound and a polymer of a quaternary ammonium salt having a cyclic structure.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An electro-deposited copper foil obtained by electrolysis of a copper electrolytic solution, wherein a tensile strength as received (hereinafter referred to as a “tensile strength as received”) is 88.4 kgf/mm 2 to 100 kgf/mm 2 , wherein a tensile strength after heating at 180° C. for 60 minutes (hereinafter referred to as a “tensile strength after heating”) is 85% or more of the tensile strength as received.

  2. Claim 2Depends on #1

    The electro-deposited copper foil according to claim 1 , wherein a tensile strength as received measured at 30 days after manufacturing is not less than 65 kgf/mm 2 .

  3. Claim 3Depends on #1

    The electro-deposited copper foil according to claim 1 , wherein an elongation as received (hereinafter referred to as an “elongation as received”) is 3% to 15%.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (22)

PatentTitleYearCitations
US 5,431,803 AElectrodeposited copper foil and process for making same199583
JP H07188969 AElectrodeposited copper foil and its preparation—39
WO 9,743,466 A1High-tensile electrolytic copper foil and process for producing the same—21
JP H10330983 AElectrolytic copper foil and its production—45
US 5,863,666 AHigh performance flexible laminate199944
JP H11501268 A高性能の可撓性積層体—8
US 5,958,209 AHigh tensile strength electrodeposited copper foil and process of electrodepositing thereof199930
US 6,194,056 B1High tensile strength electrodeposited copper foil200112
JP 2001123289 AElectrolytic copper foil and method for manufacturing the same—32
US 6,231,742 B1Electrolytic Copper foil and process for producing the same200133
JP 2001329390 AElectrolyzer of electrolytic copper foil and electrolytic copper foil obtained in the electrolyzer—20
US 6,652,725 B2Electrodeposition apparatus for producing electrodeposited copper foil and electrodeposited copper foil produced by the apparatus20034
WO 2004/055246 A1Copper electrolytic solution and electrolytic copper foil produced therewith—10
US 2004163842 A1Flexible printed wiring board for chip-on-film—51
JP 2004263289 ALow rough surface electrolytic copper foil, and production method therefor—27
WO 2004/101859 A1Low surface roughness electrolytic copper foil and process for producing the same—6
JP 2004339558 ALow rough surface electrolytic copper foil, and its production method—23
JP 2006152420 AElectrolytic copper foil and method for producing the same—43
US 2006166032 A1Copper electrolytic solution and electrolytic copper foil produced therewith—9
US 2006191798 A1Electrolytic copper foil with low roughness surface and process for producing the same—16
US 2006210823 A1Low surface roughness electrolytic copper foil and process for producing the same—18
US 7,789,976 B2Low surface roughness electrolytic copper foil and process for producing the same20108

Non-Patent Literature (5)

  • English language Abstract JP 07-188969.
  • English language Abstract JP 10-330983.
  • English language Abstract JP 2001-123289.
  • English language Abstract JP 2001-329390.
  • English language Abstract JP 2004-263289.