Patents
US 7,789,976 B2#12938006 Most CitedExpiredUnited States (USPTO)Utility

Low surface roughness electrolytic copper foil and process for producing the same

8Forward Citations (#12938006 Global)
0.5/yrCitation Velocity (#15311951 Global)
2.17Citation PageRank (#12744646 Global)
12Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An electrodeposited copper foil with low surface roughness having a surface roughness R z not higher than 2.5 μm and an elongation percentage not smaller than 6% at 180° C. in which tensile strength at 25° C. measured within 20 min of the point in time of ending electrodeposition is not higher than 500 MPa and the lowering rate of tensile strength at 25° C. measured within 300 min of the point in time of ending electrodeposition is not higher than 10%. The electrodeposited copper foil with low surface roughness is produced by a process employing aqueous solution of sulfuric acid-copper sulfate as electrolyte and conducting a DC current between an insoluble anode of titanium coated with a platinum metal element or its oxide element and a titanium cathode drum facing the anode, wherein the electrolyte contains hydroxyethylcellulose, polyethyleneimine, a sulfonate of active organic sulfur compound, acetylene glycol and chlorine ions.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 8.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An electrodeposited copper foil with low surface roughness, comprising a matte side roughness Rz of an electrodeposited copper foil is 2.5 μm or less, a tensile strength at 25 ° C. measured within 20 minutes from completion of electrodeposition is 880 MPa or higher and, at the same time, a lowering rate of a tensile strength at 25° C. measured after 300 minutes from completion of electrodeposition is 10% or lower.

  2. Claim 2Independent Claim

    An electrodeposited copper foil with low surface roughness, comprising a matte side roughness Rz of an electrodeposited copper foil is 2.5 μm or lower, a tensile strength at 25° C. measured within 20 minutes from completion of electrodeposition is 880 MPa or higher and, at the same time, a lowering rate of a tensile strength at 25° C. measured after heat treatment at 100° C. for 10 minutes from completion of electrodeposition is 10% or lower.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗