Patents
US 9,302,938 B2#27251974 Most CitedActiveUnited States (USPTO)Utility

Strengthened glass and methods for making using differential density

4Forward Citations (#27251974 Global)
0.4/yrCitation Velocity (#20186105 Global)
1.06Citation PageRank (#38342951 Global)
26Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Chemically strengthened glass and a method for making utilizing differential areal density are provided. The method includes providing a substrate having a glass chemical structure. Host alkali ions are situated in the chemical structure. The substrate has a treatment-rich volume and a treatment-poor volume located as opposed to each other in the substrate. The method also includes providing an exchange medium characterized by having an areal density, associated with an ion exchange rate, of invading alkali ions having an average ionic radius that is larger than an average ionic radius of the host alkali ions. The method also includes providing a modified exchange medium characterized by having a modified areal density, associated with a modified ion exchange rate, of the invading alkali ions. The method also includes applying the exchange mediums and conducting ion exchange to produce the strengthened substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for making a strengthened substrate, the method comprising: applying an exchange medium to a surface of a treatment-poor volume of a substrate, wherein the substrate has a glass chemical structure including host alkali ions having an average ionic radius situated in the glass chemical structure, wherein the treatment-poor volume is one of dimensional volumes included in the substrate, and wherein the exchange medium has an areal density of invading alkali ions having an average ionic radius that is larger than the average ionic radius of the host alkali ions, and the areal density is

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (26)

PatentTitleYearCitations
US 3,433,611 AStrengthening glass by multiple alkali ion exchange1969228
US 3,453,095 AOxidation method of producing glass having an increased breaking strength19699
JP S61205640 AChemical reinforcement of float glass—9
US 4,671,814 AMethod of strengthening glass article formed of float glass by ion exchange198779
US 4,859,636 AChemically strengthened glass article formed of float glass198991
JP H0927150 ASelectively chemically reinforced data storage disk and its manufacture—14
US 5,654,057 ASheet glass flattening method, method of manufacturing glass substrate for an information recording disk using flattened glass, method of manufacturing a magnetic recording disk using glass substrate, and magnetic recording medium199772
US 5,733,622 AEdge strengthened substrate of a data storage disk and method for fabricating same199853
US 6,748,765 B2Overflow downdraw glass forming method and apparatus200436
US 6,810,688 B1Method for treating glass substrates and glass substrates for the producing of display screens200429
US 2005090377 A1Lithia-alumina-silica containing glass compositions and glasses suitable for chemical tempering and articles made using the chemically tempered glass—119
US 2006075783 A1Method for strengthening flat glass plate for display—7
US 7,059,154 B1Method for making float glass, implementing device and resulting products200623
US 2009226671 A1Alkali-free glass and alkali-free glass substrate, and method of producing the same—39
US 7,743,630 B2Method of making float glass with transparent conductive oxide (TCO) film integrally formed on tin bath side of glass and corresponding product201011
WO 2011/104035 A2Chemically tempered glass—15
US 2011293928 A1Method for Strengthening Glass and Glass Using the Same—57
US 2012085130 A1Annealing of glass to alter chemical strengthening behavior—14
WO 2012/048293 A2Annealing of glass to alter chemical strengthening behavior—7
US 2012094084 A1Chemically-strengthened glass laminates—130
US 2012207980 A1Glass substrate for display and method for manufacturing the glass substrate—4
US 8,304,078 B2Chemically strengthened lithium aluminosilicate glass having high strength effective to resist fracture upon flexing201214
US 2012295072 A1Glass plate and process for producing glass plate—13
US 2012321898 A1Chemically tempered glass—80
US 2012329525 A1Glass substrate of cover glass for portable electronic device, image display unit for portable electronic device, portable electronic device and method of manufacturing glass substrate of cover glass for portable electronic device—36
US 8,507,392 B2LAS-type float glass20137

Non-Patent Literature (2)

  • International Search Report for International Application No. PCT/JP2014/060353, mailed May 13, 2014, 2 pages.
  • U.S. Appl. No. 14/808,970, filed Jul. 24, 2015, Kreski.