Chemically strengthened lithium aluminosilicate glass having high strength effective to resist fracture upon flexing

14Forward Citations (#7106069 Global)
1.0/yrCitation Velocity (#6577156 Global)
1.89Citation PageRank (#15969029 Global)
18Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Chemically strengthened lithium aluminosilicate glass is characterized by a surface compression of at least 100,000 psi and a compression case depth of at least 600 microns. The glass also may be characterized by a compression at 50 microns below a surface of the glass that is at least 30,000 psi. A method of making this glass includes providing a lithium aluminosilicate glass having a composition comprising (in weight %): Li 2 O in an amount ranging from 3 to 9%, Na 2 O+K 2 O in an amount not greater than 3%, and Al 2 O 3 in an amount ranging from 7 to 30%. The composition provides the glass with an annealing point temperature of at least 580° C. A mixed potassium and sodium salt bath is provided comprising predominantly potassium salt. A ratio of moles of sodium salt to moles of potassium salt in the mixed salt bath can range from 1:10 to 1:2. The temperature of the salt bath is maintained in a range of 450° C. up to an annealing point temperature of the glass. The glass is immersed in the salt bath for a period ranging from 2 to 96 hours. The inventive strengthened glass has high strength effective to resist fracture upon flexing and includes: bullet-resistant glass, blast-resis

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 14.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Chemically strengthened lithium aluminosilicate glass having high strength effective to resist fracture upon flexing, the glass having a composition comprising: SiO 2 and Al 2 O 3 , wherein the glass is characterized by having a surface compression of at least about 100,000 psi and a compression case depth of at least about 600 microns, wherein the glass is formed by chemically strengthening an untreated glass having a composition including Li 2 O in an amount ranging from about 3 to 9 weight % and Al 2 O 3 in an amount ranging from about 7 to 30 weight % and SiO 2 , and an annealing point t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Arun K. Varshneya, "14.8: Some aspects of Diffusion and Conduction Phenomena", Fundamentals of Inorganic Glasses, pp. 339-345.
  • Arun K. Varshneya, "18.12: Strengthening and Toughening", Fundamentals of Inorganic Glasses, pp. 444-449.
  • ASTM Designation: C 1048, "Standard specification for heat-treated flat glass-kind HS, kind FT coated and uncoated glass", pp. 356-362.
  • ASTM Designation: C 1422, "Standard specification for chemically strengthened flat glass", pp. 432-434.
  • ASTM Designation: C 158, "Standard test methods for strength of glass by flexure (determination of modulus of rupture)", pp. 20-27.