US 9,243,304 B2#43139412 Most CitedActiveUnited States (USPTO)Utility

Soft magnetic alloy and method for producing a soft magnetic alloy

2Forward Citations (#43139412 Global)
0.2/yrCitation Velocity (#33389536 Global)
0.94Citation PageRank (#45576201 Global)
14Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A soft magnetic alloy is provided that consists essentially of 47 weight percent≦Co≦50 weight percent, 1 weight percent≦V≦3 weight percent, 0 weight percent≦Ni≦0.25 weight percent, 0 weight percent≦C≦0.007 weight percent, 0 weight percent≦Mn≦0.1 weight percent, 0 weight percent≦Si≦0.1 weight percent, at least one of niobium and tantalum in amounts of x weight percent of niobium, y weight percent of tantalum, remainder Fe. The alloy includes 0 weight percent≦x<0.15 weight percent, 0 weight percent≦y≦0.3 weight percent and 0.14 weight percent≦(y+2x)≦0.3 weight percent. The soft magnetic alloy has been annealed at a temperature in the range of 730° C. to 880° C. for a time of 1 to 6 hours and comprises a yield strength in the range of 200 MPa to 450 MPa and a coercive field strength of 0.3 A/cm to 1.5 A/cm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A soft magnetic alloy consisting essentially of 47 weight percent≦Co≦50 weight percent, 1 weight percent≦V≦3 weight percent, 0 weight percent<Ni≦0.25 weight percent, 0 weight percent≦C≦0.007 weight percent, 0 weight percent≦Mn≦0.1 weight percent, 0 weight percent≦Si≦0.1 weight percent, niobium in an amount of x weight percent of niobium, remainder Fe, wherein Zr is present in an amount of not more than 0.5 weight percent, wherein 0.07 weight percent≦x<0.125 weight percent, wherein the alloy has been annealed at a temperature in the range of 730° C. to 880° C. for a time of 1 to 6 hours,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • A.V. Major et al., "High Saturation Ternary Cobalt-Iron Based Alloys", IEEE Transactions on Magnetics, vol. 24, No. 2, Mar. 1988, pp. 1856-1858.
  • German Examination Report for App. No. 10 2012 105 606.5 dated Nov. 3, 2014.