The invention relates to a laminated core with soft-magnetic material and to a method for joining core laminations by adhesive force to form a soft-magnetic laminated core. The laminated core comprises core laminations made of soft-magnetic sheets, which form a core lamination…
Pieper Witold
The invention relates to a laminated core (1) having a soft magnetic material (3) and to a method for joining core sheets (4) in a bonded manner to form a soft-magnetic laminated core (1). The laminated core (1) comprises core sheets (4) made of soft-magnetic plates (5), which…
The invention relates to a method for the production of a soft magnetic core for generators and generator with a core of this type. To produce a core, a plurality of magnetically activated and/or magnetically activatable textured laminations is produced from a CoFeV alloy. This…
A soft magnetic alloy consists essentially of 5 percent by weight≦Co≦30 percent by weight, 1 percent by weight≦Cr≦20 percent by weight, 0.1 percent by weight≦Al≦2 percent by weight, 0 percent by weight≦Si≦1.5 percent by weight, 0.017 percent by weight≦Mn≦0.2 percent by weight,…
A soft magnetic alloy is provided that consists essentially of 47 weight percent≦Co≦50 weight percent, 1 weight percent≦V≦3 weight percent, 0 weight percent≦Ni≦0.25 weight percent, 0 weight percent≦C≦0.007 weight percent, 0 weight percent≦Mn≦0.1 weight percent, 0 weight…
A method for joining core laminations by adhesive force to form a soft-magnetic laminated core by applying a coating that is wettable with epoxy resin to top sides and undersides of each sheet. The sheets are separated into core laminations made of soft-magnetic sheets, which…
The soft magnetic alloy contains cobalt (in weight%) (10-22), vanadium (0-4), chromium (1.5-5), manganese (1-2), molybdenum (0-1), silicon (0.5-1.5), aluminum (0.1-1), and remainder of iron. The soft magnetic alloy contains cobalt (in weight%) (10-22), vanadium (0-4), chromium…
A sensor comprises a magnetic field source, at least one flux conducting soft magnetic element with at least one air gap and at least one magnetic field sensor located in the air gap and measuring a change of the magnetic field of the magnetic field source. The flux conducting…
The invention relates to a method for production of a soft-magnetic core for generators and a generator comprising such a core. A number of magnetically-formed or magnetically-formable sheets of a CoFeV alloy with a texture are produced for the production of a core. The number…
Die Erfindung betrifft eine Vorrichtung zum Wärmetausch (1), die einen steifen äußeren Ring (1), einen flexiblen inneren Ring (2), elastokalorische Elemente (3), die radial zwischen dem äußeren Ring (1) und dem inneren Ring (2) gespannt sind und ein rotierendes Formelement (4)…
A soft magnetic alloy comprises (by weight): 10-22% Co, 0-4 % V, 1.5-5 % Cr, 0 <Mn < 1 %, 0-1 % Mo, 0.5-1.5 % Si, 0.1-1.0 % Al, and the remainder iron. The total amount of chromium, manganese, molybdenum, aluminium, silicon and vanadium lies in the range 4.0-9.0 %. The…
Die Erfindung betrifft ein Verfahren zur Herstellung eines Verbundblechpakets (3). Dieses umfasst das Bereitstellen eines gestapelten Schichtpakets (2) aus abwechselnd aufeinanderfolgenden ersten Schichten (11) mit einer ersten Dicke (d1) im Bereich von 0,1 mm bis 1,0 mm und…
Es wird ein Stator (16) für eine elektrische Maschine (10), eine elektrische Maschine (10) und ein Herstellungsverfahren vorgeschlagen. Der Stator (16) weist einen ringförmigen Statorkörper (18) und Statorzähne (22) auf, welche an dem Statorkörper (18) angeordnet sind, wobei der…
Disclosed are soft magnetic alloys that consist essentially of 10% by weight≦Co≦22% by weight, 0% by weight≦V≦4% by weight, 1.5% by weight≦Cr≦5% by weight, 1% by weight≦Mn≦2% by weight, 0% by weight≦Mo≦1% by weight, 0.5% by weight≦Si≦1.5% by weight, 0.1% by weight≦Al≦1.0% by…
A soft magnetic alloy is provided that consists essentially of 47 weight percent ≦Co≦50 weight percent, 1 weight percent V≦3 weight percent, 0 weight percent ≦Ni≦0.2 weight percent, 0.08 weight percent ≦Nb≦0.12 weight percent, 0 weight percent ≦C≦0.005 weight percent, 0 weight…
Die Erfindung betrifft ein Verfahren zur Herstellung eines weichmagnetischen Kerns für Generatoren sowie einen Generator mit einem deratigen Kern. Dabei wird für das Herstellen eines Kerns eine Vielzahl magnetisch formierter und/oder magnetisch formierbarer Bleche einer…
The surface region (1, 2, 3) of the workpiece (10) has a wear-resistant layer (4). The core is made of soft magnetic material (7), which is novel in being a crystalline iron-cobalt alloy. The wear-resistant layer includes one or more of the following: chromium, nickel, carbon-…
Die Erfindung betrifft eine Vorrichtung zum Wärmetausch, die eine Wärmequelle (1), eine Wärmesenke (2), zumindest ein elastokalorisches Element (5), zumindest ein Magnetjoch (3) und zumindest einen Magnetanker (4) umfasst, wobei das Magnetjoch (3) und der Magnetanker (4) einen…
A soft magnetic alloy consists essentially of 10 percent by weight ≦Co≦22 percent by weight, 0 percent by weight ≦V≦4 percent by weight, 1.5 percent by weight ≦Cr≦5 percent by weight, 0 percent by weight <Mn<1 percent by weight, 0 percent by weight ≦Mo≦1 percent by weight,…
Manufacture method, magnetic material, Hard Magnetic, motor, starter and the generator of magnetic material.The present invention relates to a kind of methods for manufacturing magnetic material, include the following steps: i) to compress first magnetic powder and second…
The present invention relates to a thermally deformable magnet and a method of manufacturing the same.
Die Erfindung betrifft eine Vorrichtung zum Wärmetausch, welche eine Wärmequelle (7) und eine Wärmesenke (8), einen Wärmetauscher (5), der abwechselnd mit der Wärmequelle (7) und der Wärmesenke (8) verbindbar ist und ein barokalorisches Element (3), welches mit dem Wärmetauscher…
Eine weichmagnetische Legierung besteht im Wesentlichen aus 10 Gew.-% <= Co <= 22 Gew.-%, 0 Gew.-% <= V <= 4 Gew.-%, 1,5 Gew.-% <= Cr <= 5 Gew.-%, 0 Gew.-% < Mn < 1 Gew.-%, 0 Gew.-% <= Mo <= 1 Gew.-%, 0,5 Gew.-% <= Si <= 1,5 Gew.-%, 0,1 Gew.-%…
Verfahren zur Herstellung von Graphenfasern oder -bändern durch ein Spinnverfahren, das Spinnverfahren umfassend die Schritte,a. Bereitstellen einer Spinnlösung (1), in der Graphen- und/oder Graphenoxidplättchen (2) dispergiert sind, wobei die Graphen- und/oder…
Die Erfindung betrifft ein Verfahren zur Herstellung eines Elektroblechpakets (71). Diese umfasst das Herstellen eines Ausgangselektroblechpakets (40) aus einem Elektroblechstreifen mittels Hochkantrollen, das Beschichten von Blechlagen (510, 520, 530) des…