Barrier film for semiconductor wiring, sintered compact sputtering target and method of producing the sputtering target

2Forward Citations (#45273142 Global)
0.2/yrCitation Velocity (#35864444 Global)
0.87Citation PageRank (#49657397 Global)
25Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Provided are a barrier film for a semiconductor wiring containing Ni with its remainder being W and unavoidable impurities and having a composition of WxNiy (70≦x≦90, 10≦y≦30 unit: atomic percent), and a sintered compact sputtering target for forming a barrier film for a semiconductor wiring containing Ni with its remainder being W and unavoidable impurities and having a composition of WxNiy (70≦x≦90, 10≦y≦30, unit: atomic percent), and comprising a target structure configured from a W matrix and Ni particles existing therein and in which W is diffused in the Ni particles. The present invention aims to provide a sputtering target that is particularly effective for use in forming a barrier film in which the target itself has the same composition as the barrier film without depending on the nitriding reaction in the sputtering process, which is capable of effectively preventing the reaction of a semiconductor device, which is free from the generation of particles in the sputtering process, and which yields superior characteristics upon forming the barrier film, as well as a method of producing such a target.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A sintered compact sputtering target for forming a barrier film for a semiconductor wiring consisting of Ni, W and unavoidable impurities, having a composition of WxNiy (70 at %≦x≦90 at %, 10 at %≦y≦30 at %), and comprising a target structure configured from a W matrix and Ni particles dispersed therein, the Ni particles containing W diffused from the W matrix, existing as WNi particles, and having a size of 2 to 40 μm.

  2. Claim 2Depends on #1

    The sintered compact sputtering target according to claim 1 , wherein the Ni particles containing W and dispersed in the W matrix are of sizes of 2 to 5 μm and 20 to 40 μm.

  3. Claim 3Depends on #1

    The sintered compact sputtering target according to claim 1 , wherein the sintered compact sputtering target has a purity of 4N5 or higher excluding gas components.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (25)

PatentTitleYearCitations
US 3,116,146 AMethod for sintering tungsten powder196315
US 3,963,455 AElectrodeposited gold plating197619
US 3,979,209 ADuctile tungsten-nickel alloy and method for making same197621
JP S58144401 APreparation of tungsten alloy—7
JP H02163337 AManufacture of high hardness tungsten liquid phase sintered alloy—5
EP 0,496,637 A2High purity conductive films and their use in semiconductors—6
JP H06283623 ASemiconductor package—5
JP H11200025 ASputtering target material for forming tantalum silicon nitride thin film—2
JP 2000169923 ATungsten-nickel target material, electrode material, and packaging component—24
JP 2000306863 ASputtering target—12
US 6,328,927 B1Method of making high-density, high-purity tungsten sputter targets200165
JP 2003031576 ASemiconductor element and manufacturing method therefor—11
US 2003025202 A1Semiconductor device having an external electrode—63
US 2003035977 A1Barrier layer for electrical connectors and methods of applying the layer—14
JP 2003049264 ATungsten sputtering target and manufacturing method—22
JP 2003064440 AWeight made of high specific gravity high strength tungsten sintered alloy—8
US 6,815,357 B2Process and apparatus for manufacturing a semiconductor device200416
US 2006037680 A1Nickel alloy sputtering target—34
US 2009022614 A1Method for Producing Sputtering Target Material for Ni-W Based Interlayer—8
US 2009189229 A1Semiconductor devices and methods of fabricating the same—2
US 7,605,481 B2Nickel alloy sputtering target and nickel alloy thin film200915
US 7,618,505 B2Target of high-purity nickel or nickel alloy and its producing method200911
US 7,718,117 B2Tungsten sputtering target and method of manufacturing the target20104
US 7,740,718 B2Target of high-purity nickel or nickel alloy and its producing method20107
US 7,956,464 B2Sputtering target and semiconductor device manufactured using the same20115

Non-Patent Literature (3)

  • A. Kawashima et al., one page Abstract of publication titled "Characterization of Sputter-Deposited Ni-Mo and Ni-W alloy Electrocatalysts for Hydrogen Evolution in Alkaline Solution", Materials Science and Engineering A, vols. 226-228, pp. 905-909, Jun. 1, 1997.
  • AE Kaloyeros et al, one page Abstract of publication titled "Ultrathin Diffusion Barriers/Liners for Gigascale Copper Metallization", Annual Review of Materials Science, vol. 30, pp. 363-385, 2000 (month unknown).
  • M.F. Zhu et al., one page Abstract of publication titled "Amorphous Ni-N-W Film as a Diffusion Barrier between Aluminum and Silicon", Thin Film Solids, vol. 130, Nos. 3-4, pp. 245-251, Aug. 30, 1985.