Process for producing and using a W—Ni sputtering target
Abstract
A process for producing a W—Ni sputtering target includes providing the sputtering target with 45 to 75 wt % W and a remainder of Ni and common impurities. The sputtering target contains a Ni(W) phase, a W phase and no or less than 10% by area on average of intermetallic phases measured at a target material cross section.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 35 · Forward citations: 0.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A process of using a sputtering target, the process comprising the following steps: using a sputtering target having from 45 to 75% by weight of W, a balance of Ni and normal impurities, a Ni(W) phase, a W phase and no or less than 10% by area on average of intermetallic phases measured at a target material cross section, for deposition of an electrochromic layer; and producing the sputtering target by at least compacting a powder mixture of W powder and Ni powder by application of pressure, heat or pressure and heat to provide a resulting blank, and cooling the resulting blank at a cooling ra
- Claim 2Independent Claim
A process of using of a sputtering target, the process comprising the following steps: using a sputtering target having from 45 to 75% by weight
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (35)
Non-Patent Literature (1)
- Lee, S.-H., et al., “Electrochromic behavior of Ni—W oxide electrodes”, Solar Energy Materials and Solar Cells, Dec. 1995, 99. 155-166, vol. 39, Elsevier Science B.V.