A porous ceramic honeycomb article includes a primary cordierite phase and an intercrystalline glass phase. In an as-fired condition, the porous ceramic honeycomb article exhibits microcrack parameter Nb 3 ≦0.06 and an as-fired E 500° C. /E 25° C. ratio ≦0.99. The article exhibits a coated microcrack parameter Nb 3 ≦0.14 and a coated E 500° C. /E 25° C. ratio ≦1.06 after the porous ceramic honeycomb article has been washcoated and calcined at a temperature of 550° C. After the article is exposed to a thermal treatment at a temperature ≧800° C. following washcoating and calcining, at least a first portion of the porous ceramic honeycomb article has a first treated microcrack parameter Nb 3 ≧0.18, and a first treated mean coefficient of thermal expansion of not more than 12×10 −7 /° C. over a temperature range of 25° C. to 800° C. Methods of forming the porous ceramic honeycomb article are also disclosed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 7.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for forming a porous ceramic honeycomb article, the method comprising: forming a batch mixture comprising cordierite-forming raw materials, glass-forming raw materials, at least one ceramic processing aid and water; extruding the batch mixture into a green honeycomb article; firing the green honeycomb article under conditions sufficient to produce the porous ceramic honeycomb article having a primary cordierite phase and an intercrystalline glass phase, wherein, after firing, the porous ceramic honeycomb article exhibits an as-fired microcrack parameter Nb 3 ≦0.06; washcoating and cal

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,329,162 ADiesel particulate trap1982526
US 4,557,773 AMethod for selectively manifolding honeycomb structures1985150
US 4,573,896 AApparatus for selectively manifolding honeycomb structures198644
US 5,069,697 APorous ceramic honeycomb filter and method of producing the same199172
US 5,114,644 AFabrication of cordierite bodies199242
US 5,177,039 AMethod for making ceramic matrix composites199333
US 5,185,110 AMethod of producing porous ceramic filter, using cordierite composition including talc and silica powders199352
US 5,258,150 AFabrication of low thermal expansion, high porosity cordierite body1993154
US 5,275,771 AExpansion reduction of cordierite199413
US 5,409,870 AModified cordierite precursors199548
US 5,549,725 ACordierite ceramic filter199673
US 5,634,952 AExhaust gas filter and apparatus for treating exhaust gases using the same199775
US 6,080,356 ACordierite honeycomb structure and process for producing the same200010
US 6,101,793 AExhaust gas filter, method of producing the same, and exhaust gas purification apparatus200037
US 6,210,626 B1Method of producing cordierite bodies utilizing substantially reduced firing times200168
US 6,541,407 B2Cordierite body2003130
US 6,673,414 B2Diesel particulate filters200462
US 6,696,132 B2Honeycomb with varying channel size and die for manufacturing200466
US 6,752,969 B1Honeycomb structural body200413
US 6,773,481 B2Porous honeycomb filter and manufacturing method thereof2004109
US 6,803,086 B2Porous honeycomb structure body, the use thereof and method for manufacturing the same200441
US 6,809,139 B2Particulate sealant for filter plug forming200427
US 6,814,774 B2Exhaust gas purification filter200446

Non-Patent Literature (2)

  • "Global model for calculating room-temperature glass density from the composition"; Fluegel; Journal of the American Ceramics Society; 90(8)2622-2625(2007).
  • "Unified theory of thermal shock fracture initiation and crack propagation in brittle ceramics"; Materials Research Center, Allied Chemical Corporation, Morristown, NJ; Hasselman; p. 600-604; Journal of the American Ceramic Society; vol. 52, No. 11.