Patents
US 5,069,697 A#460118 Most CitedExpiredUnited States (USPTO)Utility

Porous ceramic honeycomb filter and method of producing the same

72Forward Citations (#460118 Global)
2.1/yrCitation Velocity (#1910792 Global)
16.96Citation PageRank (#439996 Global)
24Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A porous ceramic honeycomb filter having a chemical composition consisting of, as main components, 42-56 wt % SiO 2 , 30-45 wt % Al 2 O 3 , and 12-16 wt % MgO and containing cordierite as a main component of a crystalline phase. The porous ceramic honeycomb filter has a porosity of at least 40% and not greater than 55%. The volume of pores having a diameter not larger than 2 μm in the filter is not larger than 0.015 cc/g to thereby improve the collecting time with low pressure loss and high collecting efficiency.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 72.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of producing a porous ceramic honeycomb filter, comprising the steps of: mixing a cordierite raw material consisting essentially of 42-56 wt% SiO 2 , 30-45 wt% Al 2 O 3 , and 12-16 wt% MgO as main components, with a pore forming agent; adjusting a grain size of fine particles of the raw material such that a total amount of particles having a grain size not larger than 2 μm is not more than 35% of the entire wt% of the mixture; adding a plasticizer and a binder to the adjusted raw material to make a batch mixture; extrusion molding the batch mixture to produce a ceramic honeycom

  2. Claim 2Depends on #1

    The method of claim 1, wherein the total amount of particles having a grain

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗