US 8,945,498 B2#22468092 Most CitedActiveUnited States (USPTO)Utility

Method for manufacturing lithium-containing composite oxide

5Forward Citations (#22468092 Global)
0.5/yrCitation Velocity (#18127929 Global)
1.09Citation PageRank (#36976536 Global)
32Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

To simply manufacture a lithium-containing oxide at lower manufacturing cost. A method for manufacturing a lithium-containing composite oxide expressed by a general formula LiMPO 4 (M is one or more of Fe (II), Mn (II), Co (II), and Ni (II)). A solution containing Li and P is formed and then is dripped in a solution containing M (M is one or more of Fe (II), Mn (II), Co (II), and Ni (II)) to form a mixed solution. By a hydrothermal method using the mixed solution, a single crystal particle of a lithium-containing composite oxide expressed by the general formula LiMPO 4 (M is one or more of Fe (II), Mn (II), Co (II), and Ni (II)) is manufactured.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 32 · Forward citations: 5.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a lithium-containing composite oxide expressed by a general formula LiMPO 4 (M is one or more of Fe (II), Mn (II), Co (II), and Ni (II)), comprising: forming a solution containing Li and P, the solution containing Li and P being slightly alkaline; dripping the solution containing Li and P in a solution containing M (M is one or more of Fe (II), Mn (II), Co (II), and Ni (II)) while stirring the solution containing M to form a mixed solution; and performing a hydrothermal method using the mixed solution so that the lithium-containing composite oxide expressed by the g

  2. Claim 2Depends on #1

    The method for manufacturing a lithium-containing composite oxide, according to claim 1 , wherein concentrations of the solution contain

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (32)

PatentTitleYearCitations
JP H1125983 AActive material for lithium battery—162
JP 2004079276 APositive electrode activator and its manufacturing method—74
US 2004096743 A1Positive active material and non-aqueous electrolyte secondary battery—85
US 6,913,855 B2Method of synthesizing electrochemically active materials from a slurry of precursors200550
WO 2006/027925 A2Positive electrode material for non-aqueous electrolyte lithium-ion secondary battery and method for production thereof—74
JP 2006252945 AElectrode for nonaqueous electrolyte secondary battery, its manufacturing method, and nonaqueous electrolyte secondary battery—39
JP 2007103339 ANonaqueous electrolyte secondary battery—76
WO 2008/077447 A1SYNTHESIS OF ELECTROACTIVE CRYSTALLINE NANOMETRIC LiMnPO4 POWDER—35
US 2008248382 A1Deposited Microarchitectured Battery and Manufacturing Method—40
US 2008268339 A1Active material, electrode, battery, and method of manufacturing active material—48
US 2009197174 A1Synthesis of Electroactive Crystalline Nanometric LiMnPO4 Powder—23
US 7,718,314 B2Cathode material and battery201023
US 2010163790 A1Oxide coatings on lithium oxide particles—40
WO 2010/082402 A1Positive electrode active material for lithium secondary battery, and lithium secondary battery—13
US 2010202951 A1Method for the preparation of a lithium phosphate compound with an olivine crystal structure—19
US 2010227221 A1Preparation Method of Lithium-Metal Composite Oxides—40
US 2010279117 A1Electrode active composite materials and methods of making thereof—62
US 2011195310 A1Production method for electrode for battery, electrode produced by production method, and battery including electrode—24
JP 4,767,798 B2電極材料の製造方法、リチウムの回収方法、正極材料及び電極並びに電池20118
US 2011223482 A1Positive electrode for lithium secondary battery and lithium secondary battery—39
US 8,053,075 B2Crystalline ion-conducting nanomaterial and method for the production thereof20115
US 2011274975 A1Positive active material for lithium secondary battery, and lithium secondary battery—10
CN 102,315,450 AHydrothermal synthesis preparation method of ion-doped high-performance lithium iron phosphate—21
US 8,097,362 B2Electrode active material and manufacturing method of same20125
US 2012028122 A1Positive active material for lithium secondary battery and lithium secondary battery—6

Non-Patent Literature (5)

  • "Hydrothermal synthesis of LiFePO4 with small particle size and its electrochemical properties," Akira Kuwahara et al. J. Electroceram (2010), 24, pp. 69-75.
  • Dokko et al., "Electrochemeical Properties of LiFePO4 Prepared via Hydrothermal Route", Journal of Power Sources, Mar. 20, 2007, vol. 165, No. 2, pp. 656-659.
  • Kang et al., "Battery Materials for Ultrafast Charging and Discharging", Nature, vol. 458, No. 12, Mar. 12, 2009, pp. 190-193.
  • Liang et al., "Anisotropy in Magnetic Properties and Electronic Structure of Single-Crystal LiFePO4", Physical Review B, 2008, vol. 77, pp. 064414-1-064414-12.
  • Tannai et al., "Optimization of Hydrothermal Synthesis Process and Evaluation of LiFePO4 Cathode for Rechargeable Lithium Batteries", The 48th Battery Symposium in Japan, Nov. 13, 2007, pp. 66-67.