Patents
US 10,985,369 B2#32605673 Most CitedActiveUnited States (USPTO)Utility

Method for manufacturing positive electrode active material, and lithium ion battery

3Forward Citations (#32605673 Global)
0.6/yrCitation Velocity (#13382761 Global)
1.09Citation PageRank (#37016838 Global)
34Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A composite oxide with high diffusion rate of lithium is provided. Alternatively, a lithium-containing complex phosphate with high diffusion rate of lithium is provided. Alternatively, a positive electrode active material with high diffusion rate of lithium is provided. Alternatively, a lithium ion battery with high output is provided. Alternatively, a lithium ion battery that can be manufactured at low cost is provided. A positive electrode active material is formed through a first step of mixing a lithium compound, a phosphorus compound, and water, a second step of adjusting pH by adding a first aqueous solution to a first mixed solution formed in the first step, a third step of mixing an iron compound with a second mixed solution formed in the second step, a fourth step of performing heat treatment under a pressure more than or equal to 0.1 MPa and less than or equal to 2 MPa at a highest temperature more than 100° C. and less than or equal to 119° C. on a third mixed solution formed in the third step with a pH of more than or equal to 3.5 and less than or equal to 5.0.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 34 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a positive electrode active material comprising lithium, phosphorus, iron, and oxygen, comprising steps of: forming a first mixed solution by mixing a lithium compound, a phosphorus compound, and a solvent; forming a second mixed solution by adjusting pH by adding a first aqueous solution to the first mixed solution; forming a third mixed solution by mixing an iron compound with the second mixed solution after the step of forming the second mixed solution; and performing heat treatment on the third mixed solution, wherein a pH of the third mixed solution is more than

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (34)

PatentTitleYearCitations
JP 2004095385 AMethod of manufacturing positive electrode material for lithium ion battery and lithium ion battery—49
JP 2008066019 AManufacturing method of electrode material, recovery method for lithium, positive electrode material, electrode, and battery—69
WO 2008/091578 A1Wet air oxidation process using recycled catalyst—13
JP 2009301813 AMethod for manufacturing carbon-olivine type iron lithium phosphate complex, and cathode material for lithium ion battery—44
JP 2010168230 ALithium phosphate powder, slurry containing lithium phosphate, method for producing electrode active material and lithium ion battery—13
JP 2010251302 AManufacturing method of positive electrode active material for lithium ion battery, positive electrode active material for lithium ion battery and electrode for lithium ion battery, as well as lithium ion battery—71
US 2011031105 A1Manufacturing method for positive electrode active material—39
JP 2011071018 AManufacturing method for lithium ion battery positive active material, and positive active material for lithium ion battery—37
CN 102,044,666 AMethod for preparing lithium iron phosphate composite material for lithium cells—44
JP 2011181452 AManufacturing method of lithium ion battery positive electrode active material, and electrode for lithium ion battery, and lithium ion battery—30
EP 2,413,402 A1Method for producing positive electrode active material for lithium ion battery, positive electrode active material for lithium ion battery, electrode for lithium ion battery, and lithium ion battery—22
US 2012237426 A1Method for manufacturing lithium-containing composite oxide—15
JP 2012211072 AMethod for preparing lithium-containing composite oxide—8
WO 2013/031929 A1Method of manufacturing positive electrode active material for lithium ion battery—2
JP 2013054922 APositive electrode active material for secondary battery—7
JP 2013065551 AMethod for manufacturing positive electrode active material for lithium ion battery—14
US 8,470,477 B2Method of manufacturing positive electrode active material for lithium ion battery201325
US 8,501,011 B2Wet air oxidation process using recycled catalyst201315
US 8,685,570 B2Method of manufacturing positive electrode active material for lithium ion battery20148
JP 2014179176 AElectrode material and process of manufacturing the same—19
US 2014295281 A1Lithiated Manganese Phosphate and Composite Material Comprising Same—6
US 8,945,498 B2Method for manufacturing lithium-containing composite oxide20155
US 2015099159 A1Positive electrode active material, nonaqueous electrolyte battery, and battery pack—20
US 2015125751 A1Method for manufacturing lithium-containing composite oxide—11
US 9,118,077 B2Manufacturing method of composite oxide and manufacturing method of power storage device20155
US 9,216,907 B2Method of manufacturing positive electrode active material for lithium ion battery, positive electrode active material for lithium ion battery, electrode for lithium ion battery, and lithium ion battery20153
US 9,249,524 B2Manufacturing method of composite oxide and manufacturing method of power storage device20165

Non-Patent Literature (1)

  • Borong W. et al, “LiFePO4 Cathode Material”, Electric Vehicles The Benefits and Barriers, Dr. S. Soylu (Ed), 2011, pp. 199-216.