Abstract

Provided is a welding metal in which a predetermined chemical component composition is satisfied, the A value as specified by formula (1) is 3.8% to 9.0%, and the surface area percentage of carbide having a circle-equivalent diameter of 0.20 μm or greater in the welding metal is 4.0% or less. A value=0.8×[C]−0.05×[Si]+0.5×[Mn]+0.5×[Cu]+[Ni]−0.5×[Mo]+0.2×[Cr] (1) (Provided that [C], [Si], [Mn], [Cu], [Ni], [Mo] and [Cr] are the C, Si, Mn, Cu, Ni, Mo and Cr content (by mass percent), respectively) The welding metal is useful as a material for a pressure vessel of a nuclear power plant as the welding metal is high in strength and has good low-temperature toughness and drop-weight characteristics.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A welding metal, comprising: C of 0.02% to 0.10%; Si of greater than 0% to 0.50%; Mn of 1.0% to 1.9%; Ni of 2.7% to 8%; Cr of greater than 0% to 0.8%; Mo of greater than 0% to 0.8%; N of greater than 0% to 0.010%; and O of greater than 0% to 0.010%, in mass percent, wherein: a total content of Cr and Mo is from 0.10% to 1.2%; the welding metal further comprises iron and inevitable impurities; a surface area percentage of carbide having a circle-equivalent diameter of 0.20 μm or greater in the welding metal after a stress relief (SR) annealing is 4.0% or less; and an A value as specified by the

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (19)

PatentTitleYearCitations
US 4,436,554 AHigh strength and high toughness welding material198413
JP H04313488 ATig welding wire for high tension steel—7
WO 9,732,684 A1Consumable electrodes for gma welding of hsla steels—14
US 5,744,782 AAdvanced consumable electrodes for gas metal arc (GMA) welding of high strength low alloy (HSLA) steels199843
JP H11138293 ATig welding wire for cryogenic steel and its welding method—11
JP H11192555 AMethod for submerged arc welding—14
US 6,110,301 ALow alloy build up material200010
JP 2001113374 ASteel pipe having hyper strength and excellent low temperature tenacity of seam welded part and method for manufacturing therefor—13
JP 2001335879 AWeld metal—5
JP 2004315962 AHigh strength weld metal having excellent low temperature toughness—20
US 2005155960 A1Laser/arc hybrid welding process for ferritic steels—37
JP 2006257481 AHigh-strength weld metal superior in low-temperature toughness—17
JP 2008240096 AHigh strength welded steel pipe having weld metal excellent in low temperature crack resistance, and its manufacturing method—23
JP 2009101414 AWelding solid wire—15
EP 2,130,937 A1High-strength welded steel pipe having weld metal excelling in low-temperature cracking resistance and process for manufacturing the same—5
US 2010119861 A1High-strength welded steel pipe including weld metal having high cold-cracking resistance and method for manufacturing the same—4
US 8,043,407 B2Welding solid wire20113
US 2012021246 A1Weld metal and welded structure having weld joints using the same—8
US 8,124,247 B2High-strength welded steel pipe including weld metal having high cold-cracking resistance and method for manufacturing the same20124

Non-Patent Literature (2)

  • Extended European Search Report issued May 13, 2013 in Patent Application No. 11736957.9.
  • International Search Report Issued Apr. 19, 2011 in PCT/JP11/51228 Filed Jan. 24, 2011.