US 4,436,554 A#7252342 Most CitedExpiredUnited States (USPTO)Utility

High strength and high toughness welding material

13Forward Citations (#7252342 Global)
0.3/yrCitation Velocity (#24999784 Global)
4.33Citation PageRank (#4194261 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A high strength and high toughness welding material containing: C: 0.05-0.15%, Si: 0.25-0.70%, Mn: 0.60-1.80%, Ni: 4.5-11.0%, Cr: 0.20-1.20%, Mo: 0.20-0.60%, Ti: 0.03-0.12%, Cr+Mo: from 0.40% to 0.030×(Ni%) 2 by weight and the balance essentially iron.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A high strength and high toughness steel welding material which has been modified by subjecting a welding portion welded with said welding material to quenching and annealing said welding material consisting essentially of: C: 0.05-0.15%, Si: 0.25-0.70%, Mn: 0.60-1.80%, Cu: an effective amount up to 0.20%, Ni: 4.5-11.0%, Cr: 0.20-1.20%, Mo: 0.20-0.60%, Ti: 0.03-0.12%, and the balance being substantially iron and wherein the Cr+Mo is from 0.40% to 0.030×(Ni%) 2 by weight, said welding material having a yield strength ranging from 75-100 Kgf/mm 2 and having a low temperature durability of over