Preparation of industrial asphalt
Abstract
The present invention relates to a method for preparing an industrial asphalt comprising sparging an oxygen containing gas through an asphalt flux in the presence of 0.25 weight percent to about 12 weight percent of a highly saturated rubbery polymer at a temperature within the range of about 400° F. to about 550° F. for a period of time which is sufficient to increase the softening point of the asphalt flux to a value which is within the range of 185° F. to 250° F. and a penetration value of at least 15 dmm to produce the industrial asphalt. The highly saturated rubbery polymer can be a styrene-ethylene/butylene-styrene block copolymer rubber or a highly saturated styrene-ethylene/propylene-styrene block copolymer rubber.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 6.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for preparing an industrial asphalt comprising sparging an oxygen containing gas through an asphalt flux in the presence of 0.25 weight percent to 5 weight percent of a highly saturated rubbery polymer at a temperature within the range of about 400° F. to about 550° F. for a period of time which is sufficient to increase the softening point of the asphalt flux to a value which is within the range of 190° F. to 220° F. and a penetration value which is within the range of 15 dmm to 25 dmm to produce the industrial asphalt.
- Claim 2Depends on #1
The method of claim 1 wherein the asphalt flux is a hard asphalt flux.
- Claim 3Depends on #1
The method as specified in claim 1 wherein the highly saturated rubbery polymer contains repeat units of the formula: —(CH 2 —C(CH 3 ) 2 )—.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗