Blown asphalt compositions
Abstract
A process for preparing compatible, selectively hydrogenated block copolymer-modified bituminous compositions comprising blowing a mixture of the block copolymer and bitumen with an oxidizing gas at temperatures of at least 375° C. for at least 75 minutes. The modifying polymer is a selectively hydrogenated styrenic block copolymer and no blowing catalyst is required. Stable bituminous compositions comprising 6 to 25 parts by weight of block copolymer per 100 parts of asphalt are also provided as well as their application as roofing shingles.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 41 · Forward citations: 19.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for preparing a bituminous composition comprising i) heating 100 parts by weight bitumen to at least 375° F., ii) adding from 6 to 25 parts by weight of a selectively hydrogenated block copolymer having at least one A block of a polymerized monoalkenyl arene and at least one B block of a polymerized and hydrogenated conjugated diene, iii) stirring the mixture, and iv) blowing an oxygen-containing gas through the mixture at a gas flow rate of at least 5 lpm per kg of the bituminous composition for a time of at least 75 minutes in the absence of a blowing catalyst.
- Claim 2Depends on #1
The process of claim 1 wherein the selectively hydrogenated block copolymer has the general formula S-EB-S or (S-EB)nX where S is a styrene block, EB is a hydrogenated butadiene block, X is the residue of a coupling agent and n is from 2 to 8.
- Claim 3Independent Claim
The