Patents
US 8,771,816 B2#26617003 Most CitedActiveUnited States (USPTO)Utility

Controlling melt fracture in bimodal resin pipe

4Forward Citations (#26617003 Global)
0.3/yrCitation Velocity (#23271009 Global)
1.18Citation PageRank (#32998874 Global)
41Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method of preparing a medium-density polyethylene pipe comprising melting a multimodal metallocene-catalyzed polyethylene resin to form a molten polyethylene, wherein the multimodal metallocene-catalyzed polyethylene resin has a density of from about 0.925 g/ml to about 0.942 g/ml, a magnitude of slip-stick greater than about 300 psi, a stress for smooth to matte transition of greater than about 90 kPa of stress, and a shear rate for smooth to matte transition greater than about 10 s −1 , wherein the magnitude of slip-stick, stress for smooth to matte transition, and shear rate for smooth to matte transition are determined by a capillary rheology test; and forming the molten polyethylene resin into pipe. A pipe prepared from a multimodal metallocene-catalyzed polyethylene resin having a density of from about 0.925 g/ml to about 0.942 g/ml, a magnitude of slip-stick greater than about 300 psi; a stress for smooth to matte transition of greater than about 90 kPa, and a shear rate for smooth to matte transition greater than about 10 s −1 , wherein the magnitude of slip-stick, stress for smooth to matte transition, and shear rate for smooth to matte transition are determined by a cap

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 41 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of preparing a medium-density polyethylene pipe comprising: melting a multimodal metallocene-catalyzed polyethylene resin to form a molten polyethylene, wherein the multimodal metallocene-catalyzed polyethylene resin has a density of from about 0.925 g/ml to about 0.942 g/ml, a magnitude of slip-stick greater than about 300 psi, a stress for smooth to matte transition of greater than about 90 kPa of stress, and a shear rate for smooth to matte transition greater than about 10 s −1 , wherein the magnitude of slip-stick, stress for smooth to matte transition, and shear rate for smooth t

  2. Claim 2Depends on #1

    The method of claim 1 wherein the polyethylene resin has a density of from about 0.928 g/ml to about 0.940 g/ml.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (41)

PatentTitleYearCitations
US 3,248,179 AMethod and apparatus for the production of solid polymers of olefins19661,057
US 3,920,782 ASharkskin197539
US 4,187,269 AExtrusion process for reducing melt fracture198015
US 4,267,146 AMethod for reducing melt fracture during extrusion of ethylene polymers198126
US 4,282,177 AMethod for reducing sharkskin melt fracture during extrusion of ethylene polymers198129
US 4,348,349 AMethod for reducing melt fracture during extrusion of a molten narrow molecular weight distribution, linear, ethylene copolymer198232
US 4,360,494 AProcess for reducing melt fracture during extrusion of a molten narrow molecular weight distribution, linear, ethylene copolymer198223
US 4,501,885 ADiluent and inert gas recovery from a polymerization process1985757
US 4,522,776 AProcess for substantially eliminating surface melt fracture when extruding ethylene polymers198512
US 4,552,712 AProcess for reducing surface melt fracture during extrusion of ethylene polymers198515
US 4,554,120 AProcess for eliminating surface melt fracture during extrusion of thermoplastic polymers198516
US 4,588,790 AMethod for fluidized bed polymerization19861,632
US 4,713,205 AMethod for reducing melt fracture during extrusion of linear polyethylene homopolymers and copolymers by varying the geometry of the die exit face19879
US 4,948,543 AProcess for eliminating surface melt fracture during extrusion of thermoplastic polymers199025
US 5,204,032 AProcess for substantially eliminating surface melt fracture during extrusion of thermoplastic polymers19936
US 5,210,142 AReduction of melt fracture in linear polyethylene199329
US 5,320,798 AMethod for processing polyolefins at high shear rates199417
US 5,352,749 AProcess for polymerizing monomers in fluidized beds19941,434
US 5,436,304 AProcess for polymerizing monomers in fluidized beds19951,069
US 5,455,314 AMethod for controlling removal of polymerization reaction effluent1995438
US 5,459,187 APolyethylene with reduced melt fracture199513
US 5,550,193 AMelt fracture elimination in film production199648
US 5,565,175 AApparatus and method for producing ethylene polymer1996688
US 5,575,979 AProcess and apparatus for separating diluents from solid polymers utilizing a two-stage flash and a cyclone separator1996648
US 5,854,352 AMelt fracture reduction199824
US 6,100,320 AProcess for making thermoplastic profiles having reduced melt fracture200011

Non-Patent Literature (5)

  • Aaltonen, Päivi, et al., "Synthesis of functional polyethylenes with soluble metallocene/methylaluminoxane catalyst," Macromolecules, 1995, pp. 5353-5357, vol. 28, No. 15, American Chemical Society.
  • Ansari, Mahmoud, et al., "Melt Fracture of Two Broad Molecular Weight Distribution High-Density Polyethylenes," XP055110091, Polymer Engineering and Science, 2012, pp. 795-804, Society of Plastics Engineers.
  • Ansari, Mahmoud, et al., "Rheology of Ziegler-Natta and metallocene high-density polyethylenes: broad molecular weight distribution effects," Rheol Acta, 2011, pp. 17-27, vol. 50, Springer-Verlag.
  • Ansari, Mahmoud, et al., "Slip effects in HDPE flows," Journal of Non-Newtonian Fluid Mechanics, XP028340589, 2012, pp. 18-29, vol. 167-168, Elsevier B.V.
  • Blyler, Jr., L. L., et al., "Capillary flow instability of ethylene polymer melts," Polymer Engineering and Science, Jul. 1970, pp. 193-203, vol. 10, No. 4.