Process for substantially eliminating surface melt fracture during extrusion of thermoplastic polymers
Abstract
A process for substantially eliminating surface melt fracture during extrusion of a thermoplastic polymer such as a molten narrow molecular weight distribution, linear, ethylene copolymer, by incorporating into the thermoplastic polymer a wood rosin or wood rosin derivative.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 6.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for substantially eliminating surface melt fracture during extrusion of narrow molecular weight distribution, linear ethylene copolymer under conditions of flow rate and melt temperature which would otherwise produce such melt fracture which comprises incorporating into said ethylene copolymer a wood rosin or a wood rosin derivative and thereafter extruding said ethylene copolymer containing said rosin or wood rosin derivative, said rosin or wood rosin derivative being employed in an amount sufficient to substantially eliminate surface melt fracture during extrusion of said ethylene
- Claim 2Depends on #1
A process according to claim 1 wherein said ethylene copolymer is subjected to an inert gas to remove moisture prior to extrusion.
- Claim 3Depends on #2
A process according to claim 2 wherein said inert gas is nitrogen.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (5)
Non-Patent Literature (2)
- Harris, G. "Rosin and Rosin Derivatives." in: Encyclopedia of Chemical Technology, vol. 11, pp. 779-810.
- Harris, G. Rosin and Rosin Derivatives. in: Encyclopedia of Chemical Technology, vol. 11, pp. 779 810.