Method for making an abrasion-resistant steel plate and plate obtained
Abstract
The invention concerns a method for making an abrasion resistant steel plate having a chemical composition comprising: 0.35%≦C≦0.8%, 0%≦Si≦2%, 0%≦Al≦2%, 0.35%≦Si+Al≦2%, 0%≦Mn≦2.5%, 0%≦Ni≦5%, 0%≦Cr≦5%, 0%≦Mo≦0.50%, 0%≦W≦1.00%, 0.1%≦Mo+W/2≦0.50%, 0%≦B≦0.02%, 0%≦Ti≦2%, 0%≦Zr≦4%, 0.05%≦Ti+Zr/2≦2%, 0%≦S≦0.15%, N<0.03%; optionally from 0% to 1.5% of Cu; optionally Nb, Ta or V with Nb/2+Ta/4+V≦0.5%; optionally less than 0.1% of Se, Te, Ca, Bi or Pb; the rest being iron and impurities; the composition satisfying: 0.1%≦C*=C−Ti/4−Zr/8+7×N/8≦0.55% and 1.05×Mn+0.54×Ni+0.50×Cr+0.3×(Mo+W/2) 1/2 +K>1.8, with K=0.5 if B≧0.0005% and K=0 if B<0.0005% and Ti+Zr/2−7×N/2≧0.05%; hardening after austenitization while cooling at a speed>0.5° C./s between a temperature>AC 3 and ranging between T=800−270×C*−90×Mn−37×Ni−70×Cr−83×(Mo+W/2) and T−50° C.; then at a core speed Vr<115×ep −1.7 between T and 100° C., (ep=plate thickness in mm); cooling down to room temperature. The invention also concerns the resulting plate.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
05×Mn+0.54×Ni+0.50×Cr+0.3×(Mo+W/2) 1/2 +K>1.8, wherein K=0.5 if B≧0.0005% and K=0 if B<0.0005
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.