Patents
US 4,459,162 A#3146199 Most CitedExpiredUnited States (USPTO)Utility

Hot work steel

24Forward Citations (#3146199 Global)
0.6/yrCitation Velocity (#13771398 Global)
6.58Citation PageRank (#2118981 Global)
9Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A hot work steel with very high resistance to tempering and a very high strength at elevated temperatures, a good ductility and a comparatively low content of expensive alloying elements; the steel contains in weight percent: 0.30-0.45 C, 0.2-1.0 Si, 0.3-2.0 Mn, 2.0-3.5 Cr, 1.5-2.5 (W/2+Mo), 0.8-1.5 V, 0-0.01 B, balance essentially only iron and impurities in normal quantities; for a further embodiment the steel contains a maximum of 1.0, preferably a maximum of 0.5 and suitably a maximum of 0.3% cobalt; in the hardened and tempered condition the steel has a fine grain lath-martensitic or partly bainitic microstructure which is free from retained austenite, and which contains a very finely dispersed intergranular precipitation of carbides, among which vanadium carbides are the dominating carbide phase.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 24.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A hot work tool steel with a very high resistance to tempering and very high strength at elevated temperatures, a good ductility and a comparatively low content of expensive alloying elements, consisting essentially, in percent by weight, of: 0.35-0.45 C, 0.2-1.0 Si, 0.3-1.5 Mn, 2.2-3.5 Cr, 1.7-2.3 (W/2+Mo), 1.0-1.4 V, 0.001-0.01 B, and cobalt up to 0.5%, maximum, by weight where vanadium carbides are a dominating phase, balance iron and normal contents of impurities and wherein the ratio of %V/(%W/2+%Mo) is between 0.4 and 0.8.

  2. Claim 2Depends on #1

    The steel as defined in claim 1, wherein the same consists essentially, in percent by weight, of: 0.35-0.45 C, 0.2-1.0 Si, 0.3-1.5 Mn, 2.2-3.0 Cr, 1.7-2.3 (W/2+Mo), 1.0-1.4 V, 0.001-0.01 B, cobalt up to 0.5%, maximum, by weight, balance iron and normal contents of impurities, and wherein the ratio of V/(

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • Lyman, T., ed., et al., Metals Handbook, 8th Edition, vol. 7 & 8, Am. Soc. for Metals, pp. 4, 120 (vol. 7), 199 (vol. 8), TA472A3, (1973).
  • Norstrom, L., "Performance of Hot-Work Tool Steels", Scandanavian Journal of Metallurgy, vol. 11, pp. 33-38, (1982).
  • Norstrom, L., Performance of Hot Work Tool Steels , Scandanavian Journal of Metallurgy, vol. 11, pp. 33 38, (1982).