Barrier film and laminated material, container for wrapping and image display medium using the same, and manufacturing method for barrier film

0Forward Citations (#141347614 Global)
0.0/yrCitation Velocity (#141347614 Global)
0.56Citation PageRank (#141347614 Global)
18Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An object of the present invention is to provide a barrier film having the extremely high barrier property and the better transparency, a method for manufacturing the same, and a laminated material, a container for wrapping and an image displaying medium using the barrier film. According to the present invention, there is provided a barrier film provided with a barrier layer on at least one surface of a substrate film, wherein the barrier layer is a silicon oxide film having an atomic ratio in a range of Si:O:C=100:160 to 190:30 to 50, a peak position of infrared-ray absorption due to Si—O—Si stretching vibration between 1030 to 1060 cm −1 , a film density in a range of 2.5 to 2.7 g/cm 3 , and a distance between grains of 30 nm or shorter. Still more, there is provided a barrier film provided with a barrier layer on at least one surface of a substrate film, wherein the barrier layer is a silicon oxi-nitride film having an atomic ratio in a range of Si:O:N:C=100:80 to 110:40 to 70:30 to 50, a maximum peak of infrared-ray absorption due to Si—O stretching vibration and Si—N stretching vibration in a range of 900 to 1000 cm −1 , a film density in a range of 2.7 to 3.0 g/cm 3 , and a d

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a barrier film, comprising forming, as a barrier layer, a silicon oxide film having an atomic ratio in a range of Si:O:C=100:(170 to 190):(40 to 50), a peak position of infrared-ray absorption due to Si—O—Si stretching vibration between 1030 to 1060 cm −1 , a film density in a range of 2.5 to 2.7 g/cm 3 and a distance between grains of 30 nm or shorter, on a substrate film which is composed of carbonaceous resin, using either of silicon having a sintered density of 80% or higher or SiO x (‘x’ is 1 to 2) having a sintered density of 80% or higher as a film forming m

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (18)

Non-Patent Literature (3)

  • USPTO Office Action mailed Jul. 19, 2005 for parent U.S. Appl. No. 10/417,588.
  • USPTO Office Action mailed May 22, 2008 for parent U.S. Appl. No. 10/417,588.
  • USPTO Office Action mailed Nov. 1, 2004 for parent U.S. Appl. No. 10/417,588.