US 7,651,594 B2#19135275 Most CitedExpiredUnited States (USPTO)Utility

Barrier film and laminated material, container for wrapping and image display medium using the same, and manufacturing method for barrier film

5Forward Citations (#19135275 Global)
0.3/yrCitation Velocity (#25027299 Global)
2.81Citation PageRank (#8407490 Global)
4Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

An object of the present invention is to provide a barrier film having the extremely high barrier property and the better transparency, a method for manufacturing the same, and a laminated material, a container for wrapping and an image displaying medium using the barrier film. According to the present invention, there is provided a barrier film provided with a barrier layer on at least one surface of a substrate film, wherein the barrier layer is a silicon oxide film having an atomic ratio in a range of Si:O:C=100:140 to 170:20 to 40, peak position of infrared-ray absorption due to Si—O—Si stretching vibration between 1060 to 1090 cm −1 , a film density in a range of 2.6 to 2.8 g/cm 3 , and a distance between grains of 30 nm or shorter. Still more, there is provided a barrier film provided with a barrier layer on at least one surface of a substrate film, has a composition wherein the barrier layer is a silicon oxi-nitride film, and the silicon oxi-nitride film has an atomic ratio in a range of Si:O:N:C=100:60 to 90:60 to 90:20 to 40, a maximum peak of infrared-ray absorption due to Si—O stretching vibration and Si—N stretching vibration is in a range of 820 to 930 cm −1 , a film d

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 5.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a barrier film, comprising forming, as a barrier layer, a silicon oxi-nitride film having an atomic ratio of Si 100 O 60-90 N 60-90 C 20-40 , a maximum peak of infrared-ray absorption due to Si—O stretching vibration and Si—N stretching vibration is in a range of 820 to 930 cm −1 , a film density in a range of 2.9 to 3.2 g/cm 3 and a distance between grains of 30 nm or shorter, on a substrate film which is composed of resin, using silicon nitride (Si 3 N 4 ) having a sintered density of 60% or higher as a target, in the presence of an oxygen gas by a sputtering meth

  2. Claim 2Depends on #1

    The method for manufacturing a barrier film according to claim 1 , wherein the sputtering method is a RF sputtering method.

  3. Claim 3Independent Claim

    A method for manufacturing a barrier film, comprising forming, as a barrier layer, a silicon oxi-nitride film having an at

Technical Overview & Description