Abstract
A poly(arylene sulfide) resin composition including 100 parts by weight of a substantially linear straight-chain poly(arylene sulfide) resin, 1 to 50 parts by weight of a branched poly(arylene sulfide) resin having a melt viscosity of 11.0×10 4 to 27.0×10 4 Pa·s as measured at a temperature of 330° C. and a shear rate of 2 sec −1 , an average particle diameter of 50 to 2,000 μm and a melt viscoelasticity tan δ of 0.10 to 0.30 as measured at a temperature of 310° C. and an angular velocity of 1 rad/sec, and 1 to 400 parts by weight of an inorganic filler, and a production process thereof.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A poly(arylene sulfide) resin composition, comprising: (A) 100 parts by weight of a straight-chain poly(arylene sulfide) resin having a melt viscosity of 5 to 1,000 Pa·s as measured at a temperature of 310° C. and a shear rate of 1,216 sec −1 , (B) 1 to 50 parts by weight of a branched poly(arylene sulfide) resin having a melt viscosity of 11.0×10 4 to 27.0×10 4 Pa·s as measured at a temperature of 330° C. and a shear rate of 2 sec −1 , an average particle diameter of 50 to 2,000 μm and a melt viscoelasticity tan δ of 0.10 to 0.30 as measured at a temperature of 310° C. and an angular veloci
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (28)
Non-Patent Literature (2)
- EPO extended European search report dated Apr. 7, 2008.
- International Search Report for PCT/JP2005/023441 dated Mar. 20, 2006.