Patents
US 5,268,451 A#10194691 Most CitedExpiredUnited States (USPTO)Utility

Process for the preparation of cross-linked polyarylene sulfide

10Forward Citations (#10194691 Global)
0.3/yrCitation Velocity (#25455397 Global)
2.42Citation PageRank (#10696685 Global)
20Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention discloses a process for producing a granular polyarylene sulfide which has a high melt viscosity and a high degree of cross-linkage, becomes gel under melting and is easy to handle in the production and the fabrication thereof. The process disclosed herein comprises (1) a step (A) an initial-stage polymerization step for obtaining a polyarylene sulfide by reacting an alkali metal sulfide, a dihaloaromatic compound and a polyhaloaromatic compound, having three or more halogen substituents in a molecule, in the presence of water in an amount of 0.5 to 2.9 moles per mol of said alkali metal sulfide at a temperature in the range of 180° to 235° C. until the total conversion ratio of said dihalo- and polyhaloaromatic compounds reaches 50 to 98% and the melt viscosity of a polyarylene sulfide obtained at the end of the step becomes 5 to 5,000 poise, measured at 310° C. and a shear rate of 1,200/second; (2) a step (B) a temperature raising step in which while adjusting an amount of water to be 2.5 to 7 moles per mol of fed alkali metal sulfide, a temperature raising condition from the temperature of step (A) to 240° C. is controlled so that the melt viscosity of a po

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 10.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A granular cross-linked polyarylene sulfide prepared by reacting an alkali metal sulfide, a dihaloaromatic compound and a polyhaloaromatic compound in an organic amide solvent, comprising: (A) an initial-stage polymerization step for obtaining a polyarylene sulfide by reacting an alkali metal sulfide, a mixture of dihaloaromatic and polyhaloaromatic compounds in an amount of 0.98 to 1.3 mol containing 0.003 to 0.1 mol polyhaloaromatic compound having three or more halogen substituents in a molecule, per mol of the alkali metal sulfide, in the presence of water in an amount of 0.5 to 2.9 moles

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 3,919,177 AP-phenylene sulfide polymers1975258
US 4,116,947 ABranched arylene sulfide polymer production197846
US 4,451,640 AProcess for producing aromatic sulfide polymer198429
US 4,495,332 AProcess for producing aromatic sulfide polymers198534
US 4,514,558 AProcess for producing aromatic sulfide polymer with anhydrous amorphous vitreous complex dehalogenation agent198525
US 4,537,953 AProcess for producing aromatic sulfide polymer with alkaline earth metal oxide dehydrating agent198530
EP 0,166,368 A2Process for production of high to ultra-high molecular weight linear polyarylenesulfides—37
US 4,645,826 AProcess for production of high to ultra-high molecular weight linear polyarylenesulfides1987125
US 4,659,789 APhenylene sulfide resin compositions198718
JP S62226998 AHuman calcitonin precursor peptide and production thereof—5
US 4,699,975 AProcess for producing readily crystallizable arylenesulfide resin composition containing organic acid or anhydride198742
US 4,745,167 APolyarylene sulfide preparation in titanium reaction vessel with two distinct temperature ranges198847
US 4,761,468 AProcess for preparing polyarylene thioether having thiol/thiolate end group concentration of 10 micro mole/g or less198816
US 4,769,426 AProcess for preparation of polyarylene thioethers having high melt crystallization temperature198815
JP S63256757 AApparatus for compressing non-woven fabric—2
US 4,785,057 APara-phenylene sulfide block copolymer, process for the production of the same198830
US 4,794,164 AProcess for producing a polyarylene sulfide of excellent handling property and a polyarylene sulfide produced by the process thereof198852
US 4,812,539 APolyarylene sulfide preparation in titanium reaction vessel with two distinct temperature ranges198929
US 4,814,430 AProcess for producing poly(arylene sulfide) of reduced alkali metal content198952
US 5,200,500 AProcess for the preparation of cross-linked polyarylene sulfide199310