Patents
US 8,574,382 B2#34083020 Most CitedActiveUnited States (USPTO)Utility

Heat-resistant aluminium alloy

3Forward Citations (#34083020 Global)
0.2/yrCitation Velocity (#31071977 Global)
0.95Citation PageRank (#44946339 Global)
21Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A cold-hardening aluminum casting alloy with good thermal stability for the production of thermally and mechanically stressed cast components, wherein the alloy includes from 11.0 to 12.0 wt % silicon from 0.7 to 2.0 wt % magnesium from 0.1 to 1 wt % manganese less than or equal to 1 wt % iron less than or equal to 2 wt % copper less than or equal to 2 wt % nickel less than or equal to 1 wt % chromium less than or equal to 1 wt % cobalt less than or equal to 2 wt % zinc less than or equal to 0.25 wt % titanium 40 ppm boron optionally from 80 to 300 ppm strontium and aluminium as the remainder with further elements and impurities due to production individually at most 0.05 wt %, in total at most 0.2 wt %. The alloy is suitable in particular for the production of cylinder crank cases by the die-casting method.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A cold-hardening aluminium casting alloy for the production of thermally and mechanically stressed cast components, said alloy comprising: from 11.2 to 11.8 wt % silicon, from 0.6 to 0.9 wt % manganese, less than or equal to 0.15 wt % iron, from 0.7 to 1.0 wt % magnesium, from 1.8 to 2.0 wt % copper, from 0.5 to 1.0 wt % chromium, from 1.7 to 2.0 wt % zinc, from 0.08 to 0.25 wt % titanium, from 20 to 30 ppm boron, less than or equal to 2 wt % nickel, less than or equal to 1 wt % cobalt, optionally from 80 to 300 ppm strontium, and aluminium as the remainder with further elements and impurities

  2. Claim 2Depends on #1

    An aluminium alloy according to claim 1 for thermally and mechanically stressed cast components produced by a die-casting, moul

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 3,306,738 AAluminium alloys196710
US 3,868,250 AHeat resistant alloys197527
JP S53115407 AEngine cylinder block and the manufacture thereof—4
US 4,336,076 AMethod for manufacturing engine cylinder block198235
CN 85,102,454 AAluminium alloy for casting piston of eatectic silicon, copper, magnesium, manganese and tellurium series—5
JP H01108339 AAluminum alloy for piston combining heat resistance with high strength—7
SU 1,094,377 A1Aluminium-base castable alloy19905
RU 1,709,746 CAluminium base wear-resistant alloy19943
WO 9,615,281 A1Cast aluminium alloy—12
RU 2,067,041 C1Aluminium alloy for strengthening surface welding19964
WO 9,713,882 A1A METHOD OF REDUCING THE FORMATION OF PRIMARY PLATLET-SHAPED BETA-PHASE IN IRON CONTAINING AlSi-ALLOYS, IN PARTICULAR IN Al-Si-Mn-Fe ALLOYS—15
JP H1036933 ACast cable parts—6
JP H11513439 A鉄含有AlSi合金、特にAl−Si−Mn−Fe合金中の微小板形状の一次β相の形成を減少させる方法—10
WO 0,043,560 A1Aluminum-magnesium-silicon alloy—14
WO 0,071,772 A1Aluminum-silicon alloy having improved properties at elevated temperatures—19
EP 1,234,893 A1Cast alloy of the type AlMgSi—6
DE 10,333,103 A1Piston used in an I.C. engine is made from an aluminum cast alloy containing additions of titanium, silicon, copper, iron, nickel and phosphorus—14
FR 2,859,484 A1Cast aluminum alloy component with high flow resistance for use in turbo-charged petrol and diesel engines, e.g. pistons for internal combustion engines—11
US 2005163647 A1Aluminum-silicon alloy having reduced microporosity—39
EP 1,645,647 A1Cold age hardenable Al-alloy and process of the manufacture of a cast part—7
JP 2006322032 AAluminum alloy for semi-solid casting, and aluminum-alloy casting and its manufacturing method—20

Non-Patent Literature (1)