Method for manufacturing engine cylinder block
Abstract
Engine cylinder block made of an aluminum alloy containing in weight 4 to 14% of Si, 1 to 5% of Cu and 0.2 to 0.8% of Mg. Method for manufacturing the cylinder block includes a heat treatment step after moulding of such aluminum alloy.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 35.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
Method for manufacturing an engine cylinder block comprising the steps of moulding an aluminum alloy consisting essentially of in weight between about 4 to 14% of Si, 1 to 5% of Cu and 0.2 to 0.8% of Mg to form a blank of the cylinder block and subjecting the moulded blank to a heat treatment at between about 200° to 400° C. for between about 1 to 10 hours, followed by air cooling the blank.
- Claim 2Independent Claim
Method for manufacturing an engine cylinder block comprising the steps of moulding an aluminum alloy consisting essentially of in weight between about 4 to 14% of Si, 1 to 5% of Cu and 0.2 to 0.8% of Mg to form a blank of the cylinder block and subjecting the moulded blank to a heat treatment at a temperature of between about 480° to 550° C. for between about 4 to 10 hours, quenching the blank, heating the quenched blank to a temperature between about
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 35 total)
References Cited — Backward Prior Art (3)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 1,799,837 A | Aluminum base alloy and piston made therefrom | 1931 | 7 |
| US 1,924,726 A | Aluminum alloy | 1933 | 2 |
| US 4,055,417 A | Hyper-eutectic aluminum-silicon based alloys for castings | 1977 | 20 |