Patents
US 8,568,901 B2#34055283 Most CitedActiveUnited States (USPTO)Utility

Filler metal composition and method for overlaying low NOx power boiler tubes

3Forward Citations (#34055283 Global)
0.2/yrCitation Velocity (#31070656 Global)
0.96Citation PageRank (#44571390 Global)
22Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An alloy for use as a welding overlay for boiler tubes in a low NO x coal-fired boiler comprising in % by weight: 36 to 43% Cr, 0.2 to 5.0% Fe, 0-2.0% Nb, 0-1% Mo, 0.3 to 1% Ti, 0.5 to 2% Al, 0.005 to 0.05% C, 0.005 to 0.020% (Mg+Ca), 0-1% Mn, 0-0.5% Si, less than 0.01% S, balance substantially Ni and trace additions and impurities. The alloy provides exceptional coal ash corrosion resistance in low partial pressures of oxygen. The alloy also increases in hardness and in thermal conductivity at service temperature over time. The increased hardness improves erosion resistance of the tubes while the increased thermal conductivity improves the thermal efficiency of the boiler and its power generation capabilities.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An alloy suitable for use as a welding overlay for boiler tubes in a low NO x coal-fired boiler comprising in % by weight: 36 to less than 42% Cr, 0.2 to 5.0% Fe, 0.06 to 2.0% Nb, 0-1% Mo, 0.3 to 1% Ti, 0.5 to 2% Al, 0.005 to 0.05% C, 0.005 to 0.020% (Mg+Ca), 0-1% Mn, 0-0.5% Si, less than 0.01% S, balance substantially Ni and trace additions and impurities.

  2. Claim 2Depends on #1

    The alloy of claim 1 providing exceptional coal ash corrosion resistance in low partial pressures of oxygen.

  3. Claim 3Depends on #1

    The alloy of claim 1 in an after-welded state providing increased thermal conductivity at service temperature over time.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (22)

PatentTitleYearCitations
US 3,865,581 AHeat resistant alloy having excellent hot workabilities197594
US 3,874,938 AHot working of dispersion-strengthened heat resistant alloys and the product thereof197519
US 4,010,309 AWelding electrode1977103
US 4,025,314 ANickel-chromium filler metal19779
US 4,400,209 AAlloy for making high strength deep well casing and tubing having improved resistance to stress-corrosion cracking198349
US 4,662,920 ACast component of nickel alloys containing large amounts of chromium198718
JP H02185961 ACorrosion and erosion resistant steel tube for boiler—7
JP H06128671 AAlloy excellent in resistance to stress corrosion cracking—6
JP H0711366 AAlloy excellent in hot workability and corrosion resistance in high temperature water—15
JP H0770680 AAlloy excellent in hot workability and corrosion resistance in high temperature water—6
US 5,543,109 AHeat resistant high chromium austenitic alloy excellent in strength at elevated temperatures199632
JP H093616 APowder mixture for thermal spraying—10
JP H0952194 AWelding method of high chromium nikkel alloy member—6
JP H09108888 AMaterial for powder build-up welding—15
EP 0,909,830 A1Hot working high chromium alloy—3
US 5,958,332 ACylinder member and nickel-based facing alloys199926
US 6,106,643 AHot working high-chromium alloy200013
JP 2001239396 ANickel-group alloy covered electrode—9
CN 1,386,877 ACast Ni-base alloy for slide block of heater for rolling steel—13
US 2005045251 A1Stainless steel and stainless steel pipe having resistance to carburization and coking—17
US 2005158203 A1Nickel- based alloy with excellent corrosion resistance in inorganic-acid-containing supercritical water environment—5
JP 2008115443 ANi-BASED SELF-FLUXING ALLOY POWDER FOR THERMAL SPRAYING, ITS PRODUCTION METHOD, AND SELF-FLUXING ALLOY SPRAYED COATING OBTAINED USING THE POWDER—18

Non-Patent Literature (1)

  • Viswanathan, R. et al., "Boiler Materials for Ultra-Supercritical Coal Power Plants-Steamside Oxidation", Journal of Materials Engineering and Performance, Jun. 2006, pp. 255-274, vol. 15(3), ASM International.