Hot working high chromium alloy
Abstract
Hot working a nickel-chromium alloy that contains by weight percent, 42 to 65 chromium, 0.002 to 0.1 calcium, 0.002 to 0.1 magnesium, 0 to 2 aluminum, about 0 to 5 cobalt, 0 to 3 copper, 0 to 5 iron, 0 to 5 manganese, 0 to 3 molybdenum, 0 to 3 niobium, 0 to 2 silicon, 0 to 3 tantalum, 0 to 5 titanium, 0 to 5 tungsten, 0 to 5 vanadium, 0 to 1 zinc, 0 to 0.2 carbon 0 to 0.1 silver, 0 to 0.1 cerium, 0 to 0.1 phosphorus, 0 to 0.1 sulfur, less than 0.005 total boron, rare earths and zirconium and balance nickel and incidental impurities, at a temperature of at least 800°C improves formability for α-phase chromium alloys.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 3.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (5)
Non-Patent Literature (5)
- PATENT ABSTRACTS OF JAPAN vol. 008, no. 050 (M - 281) 7 March 1984 (1984-03-07)
- PATENT ABSTRACTS OF JAPAN vol. 009, no. 164 (M - 395) 10 July 1985 (1985-07-10)
- PATENT ABSTRACTS OF JAPAN vol. 017, no. 259 (C - 1061) 21 May 1993 (1993-05-21)
- PATENT ABSTRACTS OF JAPAN vol. 095, no. 004 31 May 1995 (1995-05-31)
- PATENT ABSTRACTS OF JAPAN vol. 095, no. 006 31 July 1995 (1995-07-31)