Production of nickel
Abstract
A method of smelting a nickel intermediate product in a smelter that contains a molten bath of metal and slag to produce a nickel product, the method comprising supplying the nickel intermediate product and a solid reductant to the smelter and smelting the nickel intermediate product to produce molten nickel, and controlling the chemistry of the slag so that the slag has (a) a high solubility for elements and compounds in the nickel intermediate product that are regarded as contaminants in the nickel product and (b) a liquidus temperature in the range of 1300-1700 C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of smelting a nickel hydroxide or nickel carbonate intermediate product in a smelter that contains a molten bath of metal and slag to produce a nickel product, the method comprising supplying the intermediate product and a solid reductant to the smelter; smelting the intermediate product to produce molten nickel; and controlling the chemistry of the slag so that the slag has (a) a solubility for contaminants including magnesium, calcium, cobalt, copper, manganese, silicon, sulfur, phosphorous and/or aluminium in elemental form or as compounds, sufficient to facilitate partitioning of
- Claim 2Depends on #1
The method of claim 1 wherein the slag has a liquidus temperature in the range of about 140
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (8)
Non-Patent Literature (1)
- Machine translation of JP 08-035022 published Feb. 6, 1996.