Patents
US 3,769,002 A#7408849 Most CitedExpiredUnited States (USPTO)Utility

Reduction of nickel and cobalt oxides in a molten metal bath of controlled oxygen content

13Forward Citations (#7408849 Global)
0.2/yrCitation Velocity (#28172195 Global)
3.05Citation PageRank (#7393049 Global)
12Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Metal oxides, including oxides of nickel and cobalt and compounds heat decomposable thereto, and a carbonaceous reductant are introduced into a turbulent bath of the corresponding metal which bath contains at least about 0.01 percent dissolved oxygen to maintain the dissolved oxygen content of the bath at at least about 0.01 percent but less than saturation, while the carbonaceous reductant reacts to generate carbon monoxide. The metal bath is maintained in the molten state by burning above the bath carbon monoxide generated in situ and hydrocarbon fuels with an excess of free oxygen. Impurities oxidizable to volatile oxides can be eliminated by subjecting the oxygen-containing bath, or a part thereof, to subatmospheric pressures, or the metal bath can be surface blown with a free oxygen-containing gas to adjust the oxygen content of the bath before subatmospheric treatment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 13.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 2Depends on #1

    The process as described in claim 1 wherein the bath contains at least about 0.1 percent dissolved oxygen but is not saturated therewith.

  2. Claim 3Independent Claim

    A process for reducing a nickel compound which comprises: establishing a turbulent nickel bath which contains at least about 0.01 percent dissolved oxygen but not saturated therewith; feeding at least one nickel compound selected from the group consisting of nickel oxide and compounds heat decomposable thereto and a carbonaceous reductant to the nickel bath while maintaining the dissolved oxygen level of the nickel bath at at least about 0.01 percent but less than saturation whereby the carbonaceous reductant reacts with the dissolved oxygen content in the nickel bath to generate carbon monoxi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗